Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (5): 13-20    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Mg CONTENT ON CREEP BEHAVIOUR OF Ni-BASE WROUGHT SUPERALLOY
KE Da'nian; ZHONG Zengyong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

KE Da'nian; ZHONG Zengyong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). EFFECT OF Mg CONTENT ON CREEP BEHAVIOUR OF Ni-BASE WROUGHT SUPERALLOY. Acta Metall Sin, 1983, 19(5): 13-20.

Download:  PDF(1539KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of addition of Mg on the creep behaviour of Ni-base wrought superalloy has been investigated. It was found that the trace Mg added may cause the alteration of continueous lath carbide into discontinueous massive one at the grain boundaries. It may also promote the spheroidization of the grain boundary carbide, decrease the diffusion coefficient of grain boundary and increase the activation energy for creep. The grain boundary energy and the boundary energy between grain boundary carbide and matrix are decreased and bonding strength of interface increased. Thus, the creep property and the creep-rupture life as well as the stress exponent of creep of the superalloy may be significantly improved by the impediment of the boundary sliding and the prevention of the nucleation and propagation of cracks.
Received:  18 May 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I5/13

1 (1978) , №11 1047.
2 (1979) , №7, 545.
3 (1978) , №11, 59.
4 (1973) , №4, 193.
5 可大年;仲增墉,冶金部钢铁研究总院学报,待发表.
6 Furillo, F. T.; Davidson J. M.; Tien, J. K., Mater. Sci. Eng., 39 (1979) , 267.
7 Ashby, M. F.; Raj, R., Conference on the Mechanics and Physics of Fracture, Organised by The Institute of Physics and the Metals Society, London, 1975, p.1/1-16/11.
No related articles found!