A COMPUTER PROGRAM FOR ANALYSIS OF ORIENTATION RELATIONSHIP BETWEEN MATRIX AND SECOND PHASE
LI Chunzhi (Beijing Institute of Aeronautical Materials)
Cite this article: 

LI Chunzhi (Beijing Institute of Aeronautical Materials). A COMPUTER PROGRAM FOR ANALYSIS OF ORIENTATION RELATIONSHIP BETWEEN MATRIX AND SECOND PHASE. Acta Metall Sin, 1983, 19(5): 102-108.

Download:  PDF(419KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A computer program for determination of orientation relationship between the second phase and the matrix is presented. Some examples are given.