OFF-AXIS TENSILE PROPERTIES OF γ/γ'-α-Mo DS EUTECTIC
by ZHANG Jinghua; ZHANG Yusheng; ZHANG Zhiya; XU Yongbo; TANG Yafun; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 20 August; 1982)
Cite this article: 

by ZHANG Jinghua; ZHANG Yusheng; ZHANG Zhiya; XU Yongbo; TANG Yafun; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 20 August; 1982). OFF-AXIS TENSILE PROPERTIES OF γ/γ'-α-Mo DS EUTECTIC. Acta Metall Sin, 1983, 19(4): 57-147.

Download:  PDF(4445KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study was made of the off-axis tensile properties of γ/γ'-a-Mo DS eutectic and of observation of the dynamic fracture process by SEM. If the loading direction deviates from the Mo fibre growth direction, the tensile strength and ductility decrease gradually. During the loading process, two types of cracking are observed: one is cracking of the fibre, and the other is delamination along the fibre-matrix interface. In plastic deformation, slip can pass through both the matrix and the fibre. As a rule, the thicker fibers are cracked earlier than the thinner ones, because they have less defects and better ductility. Delamination is the main source of final fracture.
Received:  18 April 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I4/57

1 Lemkey, F. D., Superalloys: Metallurgy and Manufacture, Proc. of the 3rd Int. Symp. on Superalloys, Eds. Kear, B. H.; Muzyka, D. R; Tien, J. K., et al., Claitor's Publ., Baton Rouge, 1976, p. 137.
2 Henry, M. F.; Jackson, M. R.; Gigliotti, M. F. X.; Nelson, P. B., NASA CR-159 416, (1979) .
3 Henry, M. F.; Jackson, M. R.; Walter, J. L., NASA CR-135 151, (1978) .
4 Nakagawa, Y. G.; Ohotomo, A.; Saiga, Y., Superalloys, Proc. of the 4th Int. Symp. on Superalloys, (1980) , Eds. Tien, J. K.; Wlodek, S. T.; Morrow, H. Ⅲ, et al., ASM, Metal Park, Ohio, 1980, p. 267.
5 Sprenger, H.; Richter, H.; Nickl, J. J., J. Mater. Sci., 11 (1976) , 2075.
6 Stoloff, N. S., Advances in Composite Materials, Ed. Piatti, G., London, Appl. Sci. Publ., 1978, p. 247.
No related articles found!
No Suggested Reading articles found!