ON THE HYDROGEN STORAGE BEHAVIOUR OF ALLOYS La_2Mg_(17) AND La_2Mg_(16)Ni
by SHEN Panwen; WANG Genshi; ZHANG Jizhi; YANG Xizeng (Nankai University; Tianjin) (Manuscript received 4 January; 1982)
Cite this article: 

by SHEN Panwen; WANG Genshi; ZHANG Jizhi; YANG Xizeng (Nankai University; Tianjin) (Manuscript received 4 January; 1982). ON THE HYDROGEN STORAGE BEHAVIOUR OF ALLOYS La_2Mg_(17) AND La_2Mg_(16)Ni. Acta Metall Sin, 1983, 19(4): 108-116.

Download:  PDF(503KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The hydrogen storage behaviour of the Mg-rich rare earth alloys, La_2Mg_(17) and La_2Mg_(16)Ni, has been investigated. Two plateaus related to the reactions Mg2Ni+2H_2(?)Mg_2NiH_4 and Mg+H_2(?)MgH_2 respectively exhibit in the pressurecomposition isotherm of La_2Mg_(16)Ni alloy. Partial substitution of Mg by Ni in La_2Mg_(17) gives a two-phase mixture: the major is La_2Mg_(17) type phase and the minor, Mg_2Ni type one. Hydriding of the La_2Mg_(16)Ni alloy leads to the formation of MgH_2, La hydride and Mg_2NiH_4. An experiment was also carried out on the hydrogen absorption by the alloys under either normal temperature and lower pressure or normal pressure and elevated temperature. It was found that La_2Mg_(17) and La_2Mg_(16)Ni seem to be the considerable hydrogen storage materials.
Received:  18 April 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I4/108

1 张激志;汪根时,未发表资料,1982.
2 Reilly, J. J.; Wiswall, R. H., Jr., BNL-17 136 (1972) , p.36.
3 Darriet, B.; Pezat, M.; Hbika, A.; Hagenmuller, P., Int. J. Hydrogen Energy, 5 (1980) , 173.
4 Pezat, M.; Darriet, B.; Hagenmuller, P., J. Less-Common Met., 74 (1980) , 427.
5 Yajima, S.; Kayano, H., ibid., 55 (1977) , 139.
6 Yajima, S.; Kayano, H.; Ger. Offen., 2 531 406, (1975) .
7 Muller, A., Engelhard, P.; Weisang, J. E., GB 2007202A. 1979.
8 Muller, A., ibid., GB 2007204A, 1979.
9 Darriet, B.; Hbika, A.; Pezat, M., J. Less-Common Met., 75 (1980) , 43.
10 Stampfer, J. F., Jr.; Holley, C. E., Jr.; Suttle, J. F., J. Am. Chem. Soc., 82 (1960) , 3504.
11 Reilly, J. J.; Wiswall, R. H., Jr., Inorg. Chem., 7 (1968) , 2254.
12 Korst, W. L.; Warf, J. C., ibid., 5 (1965) , 1719.
13 Farr, J. D.; Giorgi, A. L.; Bowman, M. G.; Money, R. K., J. Inorg. Nucl. Chem., 18 (1961) , 42.
14 Gavra, Z.; Mintz, M. H.; Kimmel, G.; Hadari, Z., Inorg. Chem., 18 (1979) , 3595.
15 Noreus, D.; Werner, P. E., Mater, Res. Bull., 16 (1981) , 199.
No related articles found!
No Suggested Reading articles found!