| EFFECT OF MELT SUPERHEAT ON DIRECTIONAL SOLIDIFICATION PROPERTIES OF Al-Cu ALLOY |
| by MAO Xiemin; FU Hengzhi; SHI Zhengxing; LIU Huiming (North-Western Polytechnical University. Xi'an ) |
|
Cite this article:
by MAO Xiemin; FU Hengzhi; SHI Zhengxing; LIU Huiming (North-Western Polytechnical University. Xi'an ). EFFECT OF MELT SUPERHEAT ON DIRECTIONAL SOLIDIFICATION PROPERTIES OF Al-Cu ALLOY. Acta Metall Sin, 1983, 19(3): 84-90.
|
|
|
Abstract The effect of the melt superheat on the solute distribution coefficient and the critical condition of the interface morphology on the directional solidification has been studied. It is found that the actual distribution coefficient of solute is a function of liquid state. An increase of superheat of the melt causes the increase of actual distribution coefficient for such elements of K_0<1, and the decrease of the critical conditions of G/R associated with the stability of the solid-liquid interface morphologies which seems to be available to improving the directional solidification.
|
|
Received: 18 March 1983
|
1 Tiller, W. A.; Jackson, W. A., Acta Metall., 1 (1953) , 428. 2 Chalmers, B., Principles of Solidiflcation, Wiley, New York 1964, p.158. 3 Turnbull, D., J. Chem. Phys., 18 (1950) , 198. 4 #12 5 Metals Handbook, 8th ed. Vol. 8, ASM, 1973. p.78. 6 Flemings, M. C., Solidification Processing, McGraw Hill, New York, 1974. p.78.D |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|