| EFFECT OF TRACE Cr ON PRECIPITATION AND MICROSTRUCTURAL PARAMETERS OF A COMMERCIAL PURITY Al-5.0Zn-1.8Mg ALLOY |
| by LIN Zhaoqi; FUNG Bing; SUN Guijing; YANG Shengkun (Northeast Institute of Tecknology; Shenyang) |
|
Cite this article:
by LIN Zhaoqi; FUNG Bing; SUN Guijing; YANG Shengkun (Northeast Institute of Tecknology; Shenyang). EFFECT OF TRACE Cr ON PRECIPITATION AND MICROSTRUCTURAL PARAMETERS OF A COMMERCIAL PURITY Al-5.0Zn-1.8Mg ALLOY. Acta Metall Sin, 1983, 19(3): 37-150.
|
|
|
Abstract The effect of trace Cr on the precipitation, critical nucleation temperature T_c′ and structural parameters of a commercial purity Al-5.0Zn-1.8Mg alloy has been investigated by means of hardness test, optical microscopy and TEM. It was resulted that the trace Cr may facilitate the heterogeneous precipitation and the raise of T_c′, as well as may also retard the growth of GBP, PFZ and MPt after lower temperature aging (T_a≤160℃), however, it may accelerate them after aged under elevated temperature (T_a≥180℃). The above-mentioned behaviour seems to be explained by the dual mechanism of the interaction of Cr with vacancies.
|
|
Received: 18 March 1983
|
1 Bryant, A. J., J. Inst. Met., 14 (1966) , 94. 2 Westerman, E. J.; Fetzer, M. C., J. Inst. Met., 97 (1969) , 66. 3 Truscott, J. M.; Carter, V. E.; Campbell, H. S., J. Inst. Met., 99 (1971) , 57. 4 Gruhl, W.; Cordier, H.; Brungs, U. D., Metall, 26 (1972) , 207. 5 斎藤寿雄;田中孝一,軽金属,22(1972) ,403. 6 马场义雄;高岛章,ibid.,24(1974) ,216. 7 吉田英雄;马场义雄,ibid.,31(1981) ,20. 8 Grove, C. A.; Judd, G., Metall. Trans., 4 (1973) , 1023. 9 Chen, C.; Judd, G., Metall. Trans., 9A (1978) , 553. 10 Dix, E. H., Jr., Trans. ASM, 42 (1950) , 1057. 11 Polmear, I. J.; Scott-Young, P., J. Inst. Met., 87 (1958/59) 65. 12 Thomas, G.; Nutting, J., J. Inst. Met., 88 (1959/60) . 81. 13 马场义雄,日本金属学会誌,31(1967) ,507. 14 马场义雄,ibid.,31(1967) .513. 15 铃木;(?)见;管野,軽金属,23(1973) ,126. 16 Holl, H. A., J. Inst. Met., 93 (1964/65) , 364. 17 Smith, W. F.; Grant, N. J., Metall. Trans., 2 (1971) , 1333. 18 Shastry, C. R.; Judd, G., Metall. Trans., 2 (1971) , 3283. 19 Holl, H. A., J. Inst. Met., 97 (1969) , 200. 20 Little, K.; Axon, H. J.; Hume-Rothery, W., J. Inst. Met., 75 (1949) , 39. 21 Smith, W. F.; Grant, N. J., MetalI. Trans., 1 (1970) , 1735. 22 Kelly, A.; Nicholson, R. B., Prof. Mater. Sci. 10 (1963) , 149. |
| No Suggested Reading articles found! |
|
|