Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (2): 114-117    DOI:
Current Issue | Archive | Adv Search |
NOTE ON THE PHASE DIAGRAM OF Al-Cu-Ag ALLOY SYSTEM
LIU Shuqi; ZHAO Shimin; ZHANG Qiyun (Department of Chemistry; Beijing University)
Cite this article: 

LIU Shuqi; ZHAO Shimin; ZHANG Qiyun (Department of Chemistry; Beijing University). NOTE ON THE PHASE DIAGRAM OF Al-Cu-Ag ALLOY SYSTEM. Acta Metall Sin, 1983, 19(2): 114-117.

Download:  PDF(265KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thermal analytical study of the liquidus of Al-Al_2Cu-Ag_2Al corner in the phase diagram of Al-Cu-Ag system was made if possible to ascertain a suitable fillet metal in Al brazing at medium temperature range. The system belongs to a eutectic type. The composition of the eutectic point is: Al 40.0%, Cu 19.3%, Ag 40.7% and its temperature 500℃. A phase diagram has been figured.
Received:  18 February 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I2/114

1 Goto, 引自 Mondolfo, L. F., Aluminium Alloys: Structure and Properties, Butterworths, London, 1976, p. 420.
2 McCartney, D. G.; Jordan, R. M.; Hunt, J. D., Metall. Trans., 11A (1980) , 1251.
3 Panseri, C.; Leoni, M., Alluminio, 30 (1961) , 289.
4 Cooksey, D. J. S.; Hellawell, A., J. Inst. Met., 95 (1967) , 183.
5 Yue, A. S., J. Inst. Met., 91 (1962-63) , 166.
6 Hellawell, A., Trans. Met. Soc. AIME, 233 (1965) , 1516.
7 Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 2nd ed., 1958, p. 1.
8 Hansen, M., ibid., p. 84.
9 Hansen, M., ibid., p. 18.
No related articles found!