Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (2): 106-113    DOI:
Current Issue | Archive | Adv Search |
APPLICATION OF PHASE DIAGRAMS TO SLAG ATTACK ON MgO-CaO REFRACTORIES
CHEN Zhaoyou (Luoyang Institute of Refractory Research)
Cite this article: 

CHEN Zhaoyou (Luoyang Institute of Refractory Research). APPLICATION OF PHASE DIAGRAMS TO SLAG ATTACK ON MgO-CaO REFRACTORIES. Acta Metall Sin, 1983, 19(2): 106-113.

Download:  PDF(717KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the basis of the related isothermal sections of ternary systems and the liquid or solid zones of quaternary systems at 1600℃, the attack resistance of MgO-CaO refractories has been examined with certain oxides, conventional steelmaking slags and P_2O_5-containing slags. It seems that the converter lining made of MgO-CaO refractories with a certain amount of CaO contained got the better than the MgO refractory alone to resist the attack of either conventional or P_2O_5-containing steelmaking slags.
Received:  18 February 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I2/106

1 Troemel, G.; Obst, K.-H; Goerl, E,; Stradtmann, J., Tonind.-Ztg., 90 (1966) , 193.
2 #12
3 Nafziger, R. H., High Temp. Sci., 7 (1975) , 179.
4 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Phase Diagrams for Ceramists, Second Edition, 1969, p. 209, 210, 113; Phase Diagrams for Ceramists, 1969 Supplement, p. 36, 85.
5 Johnson, R. E.; Muan, A.; J. Am. Ceram. Soc., 48 (1965) , 359.
6 Stephenson, I. M.; White, J., Trans. Br. Ceram. Soc., 66 (1967) , 443.
7 Troemel, G.; Fix, W.; Kaup. R., Arch. Eisenhuettenwes., 38 (1967) , 595.
8 Drewes, E. J.; Olette, M., ibid. 38 (1967) , 163.
9 Troemel, G.; Fix, W.; Koch, K., ibid., 38 (1967) , 177.
10 Knueppel, H.; Oeters, F., Stahl Eisen, 81 (1961) , 1437.
11 郁国城,金属学报,14(1978) ,272.
12 Troemel, G.; Koch, K., Arch. Eisenhuettenwes., 45 (1974) , 671.
13 Euler, R., Ber. Dtsch. Keram. Ges., 44 (1967) , 345.9
No related articles found!