INVESTIGATION OF HYDROGEN DISTRIBUTION IN METALS BY TRITIUM AUTORADIOGRAPHY
YANG Shixin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); YIN Wanquan (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

YANG Shixin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); YIN Wanquan (Institute of Metal Research; Academia Sinica; Shenyang). INVESTIGATION OF HYDROGEN DISTRIBUTION IN METALS BY TRITIUM AUTORADIOGRAPHY. Acta Metall Sin, 1983, 19(1): 26-140.

Download:  PDF(4118KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Tritium autoradiography was employed for the identification of: 1. the hydrogen distribution in irons with different purities; 2. the diffusion behavior uof hydrogen in metal under local load for different stress stand; 3. the distribution of tritium in the W alloys, 95%W-3.5%Ni-1.5%Fe, a kind of two-phase alloys consisted from W particles and binder of solution 54.2%Ni-27.1%Fe-20.5%W with high specific gravity and 4. the hydrogen distribution of different zones for the weld joint. It was found that the hydrogen distribution of iron is dependent on the purity of iron and the hydrogen solubility in the iron, however, grain boundary of high purity iron cannot be provided preferred sites for hydrogen accumulation site, but grain orientation difference is sensitive for tritium tracer. Tritium redistribution of hydrogen in different purity iron under different plastic deformation by the stress induced hydrogen segregation on the iron. Tritium distribution on the W-Ni-Fe sintcring alloys, even without etching, it is primarily accumulated on the interface of binding phase, which is dependent on relative solubility in two-phase alloys. The distribution of tritium on the different zone of the weld joint shows that hydrogen in the austenite weld, fusion zone. Overheat affected zone of matrix and matrix is different, which is closely connection of the carbon segregation of weld process and structure defect of matrix.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/26

1 Williams, P.; Evans, C. A., Jr., Anal. Chem., 48(1976) , 964.
2 De Oliverira, C. P.; Aucouturier, M.; Lacombe, P., Corrosion, 36(1980) , 53.
3 Ohma, H.; Tiwari, G. P.; Lijima, Y.; Hirano, K., Proceedings JIMIS-2, Hydrogen in Metals, Minakami, Gunma Perf., Japan 1979, Published by JIM, Aoba Aramaki, Japan, 1980, p. 229.
4 Taguchi, I., Proceedings JIMIS-2, Hydragen in Metals, Minakami, Gunma Perf., Japan 1979, Published by JIM, Aoba Aramaki, Japan, 1980 p. 225.
5 Aucouturier, M.; Lapasset, G.; Asoka, T., Metallography, 11(1978) , 5.
6 Louthan, M. R., Jr.; Rawl, D. E., Jr.; Huntoon, R. T., Corrosion, 28(1972) , 172.
7 Zielimski, A.; Lunarska, E.; Smialowski, M., Acta Metall., 25(1977) , 551.
8 朱桂森;刘铭成;林忠杰;俞淑延,金属学报,17(1981) ,39.
No related articles found!