DISCUSSION ON APPLICABILITY OF TENSION EQUATION IN CONTINUOUS ROLLING
Zhang Jinzhi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

Zhang Jinzhi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). DISCUSSION ON APPLICABILITY OF TENSION EQUATION IN CONTINUOUS ROLLING. Acta Metall Sin, 1982, 18(6): 755-762.

Download:  PDF(584KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An analysis and discussion were made of the evidence whether the conventional differential equation is proper to calculate the dynamic transition process. It has been proved that the equation is applicable to all continuous rolling conditions of tension less than the elastic limit, however, the error may only be introduced by the neglected term (1+σ/E). The analytical solution of the equation gives not only clarifying the physical nature of rolling practice but also improving the accuracy and amount of the dynamic analogue calculation. Combining the aforementioned conventional differential equation with the balance equation of total tension, a discrete tension formula is then derived for dynamic guage change and strip threading procedure.
Received:  18 June 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I6/755

1 张进之,钢铁,13(1978) ,№4,85.
2 张树堂;刘玉荣,钢铁,14(1979) ,№2,45.
3 张树堂;刘玉荣,金属学报,17(1981) ,206.
4 张树堂;刘玉荣,钢铁,15(1980) ,№6,34.
5 张进之,金属学报,14(1978) ,127.
6 张永光;梁国平;张进之;郑学铎,自动化学报,5(1979) ,177.
7 Bryant, G. F.; Higham, J. D,, Digital Computer Applications to Process Control. 3. , Proceedings of the Third International Conference, Ed. W. E. Miller; A. Niemi, Instrument Society of America, Pittsburgh, 1971, p. X-4.
8 有村透;鎌田正诚;斎藤森生;塑性加工,10(1969) ,29.
9 原田利夫;中岛浩卫;岸川宫一;中俣伸一;渡辺和夫;山本洋春;塑性加工,16(1975) ,60.
10 浅川基男;近藤勝也;绪方俊治;美坂佳助;松井利光;塑性加工,20(1979) ,841.
11 张进之,连轧张力系统定常性质的论证,1979(待发表).
12 田沼正也;大成幹彦,塑性加工,13(1972) ,122.
13 阿高松男;铃木弘,塑性加工,11(1970) ,676.
14 小西正躬;铃木弘,塑性加工,13(1972) ,689.
15 黄光远,自动化学报,6(1980) ,209.
16 郑学铎;张进之,未发表资料.
17 张进之;郑学铎;梁国平,钢铁,14(1979) ,№6,60
No related articles found!
No Suggested Reading articles found!