Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (6): 703-712    DOI:
Current Issue | Archive | Adv Search |
AN APPROACH TO THE ANALYSIS OF X-RAY AND ELECTRON DIFFRACTION PATTERNS OF SINGLE CRYSTALS
Pan Jinsheng (Qinghua University; Beijing)
Cite this article: 

Pan Jinsheng (Qinghua University; Beijing). AN APPROACH TO THE ANALYSIS OF X-RAY AND ELECTRON DIFFRACTION PATTERNS OF SINGLE CRYSTALS. Acta Metall Sin, 1982, 18(6): 703-712.

Download:  PDF(760KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new approach to the analysis of both X-ray and electron diffraction patterns of single crystals is presented. It consists in the rotation of the reciprocal axes of the crystal by computer.Based on this principle, a computer program, written in BASIC, is compiled for all crystal systems and has been used successfully for the indexing of both X-ray and electron diffraction patterns and the determination of crystal orientations. In addition, the same program with little modifications has been also used to plot the standard projections and simulate the Laue and electron diffraction patterns automatically.
Received:  18 June 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I6/703

1 Goehner, R. P., Advances in X-Ray Analysis, Vol. 19, Ed. Gould, R. W., Kendall/Hunt, Dubuque, Lowa, 1976, p. 725.
2 Huang, W. H.; Christensen, J. H.; Block, R. J., Metall. Trans., 2(1971) , 1367.
3 Christensen, J. H.; Huang, W. H.; Block, R. J., Metall. Trans., 2(1971) , 2295.
4 Anazia, C.; Lee, C.; Jerner, R. C. Christensen, J. H.; Peavey, J. H., Metall. Trans., 6A(1975) , 1751.
5 Ploc, R. A., J. Appl. Crystallogr., 11(1978) , 713.
6 潘金生,清华大学学报,19(1979) ,20,
7 Cullity, B. D., Elements of X-Ray Diffraction, Second Edition, Addison-Wesley, Reading, Mass., 1978, p. 340.
8 Amoros, B. D.; Buerger, M. J.; Amoros, M. C. De, The Laue Method, Academic Press, New York, 1975, p.
9 潘金生,待发表工作.
10 马莒生,金属学报,18(1982) ,64.|
No related articles found!
No Suggested Reading articles found!