EFFECT OF BORIDE ON STRESS RUPTURE PROPERTIES OF AN FeNiCr-BASE ALLOY
Zhang Jiafu; Zhou Shiwu; Cheng Xiufeng; Hu Dingan (Research Institute of Daye Steer Works; Huangshi; Hubei Province)
Cite this article: 

Zhang Jiafu; Zhou Shiwu; Cheng Xiufeng; Hu Dingan (Research Institute of Daye Steer Works; Huangshi; Hubei Province). EFFECT OF BORIDE ON STRESS RUPTURE PROPERTIES OF AN FeNiCr-BASE ALLOY. Acta Metall Sin, 1982, 18(6): 645-650.

Download:  PDF(892KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of boron on the high temperature strength of an Fe-42Ni-12Cr-4W-1. 5Mo-4.5Ti-2Al alloy has been investigated. The results indicate that the boron either soluted in solid solution or precipitated as a secondary boride phase along the grain boundaries will improve the stress rupture properties of the alloy. But the primary borides can not better it at all, moreover, it may deteriorate the high temperature strength of alloy if an overabandant primary boride occurred. It was also found that the stress rupture properties of alloy have much improved since it solution treated under elevated temperature, this seems to attribute the improvement to the increase of the amount of secondary boride precipitation at unit interface area after solutioning and aging, not to the grain growth alone from higher solution temperatures in the tested range of grain size.
Received:  18 June 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I6/645

1 北京钢铁学院,金相教研室,未发表资料,1978.
2 #12
3 金属研究所,未发表资料,1974.
No related articles found!
No Suggested Reading articles found!