INVESTIGATION OF FATIGUE CRACK GROWTH RATE FOR STEEL 16Mn
Tong Zhishen; Hou Yaoyong; Li Mingqi; Jiang Shengrui (Lanzhou University)
Cite this article: 

Tong Zhishen; Hou Yaoyong; Li Mingqi; Jiang Shengrui (Lanzhou University). INVESTIGATION OF FATIGUE CRACK GROWTH RATE FOR STEEL 16Mn. Acta Metall Sin, 1982, 18(5): 618-626.

Download:  PDF(543KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on both the calculating formula for J-integral determined by means of TPB type specimen and the experimental evidence of da/dN=C_1(ΔJ)~r ,an expression of subcritical fatigue crack growth rate characterized by AJ from TPB specimen from the linear elastic to complete yielding region has been derived as follows: For high-cycle fatigue crack, its approximate growth rate will be which seems to be identical with the Paris' relation. For high-stain fatigue crack, it may be which is analogous to the Coffin-Manson's relation.These formulae are confirmed by the experimental results for steel 16Mn specimens in the environment of atmosphere or aqueous H_2S saturated solution. It is also indicated that the aqueous H_2S saturated solution may aggravate the subcritical growth rate of fatigue cracking.
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/618

1 Coffin, L. F., Jr., Am. Soc. Test. Mater., Spec. Tech. Publ., № 520,(1973) , p. 5.
2 蔡其巩,金属学报,12(1976) ,45.
3 Dowling, N. E., Am. Soc. Test. Mater, Spec. Tech. Publ., № 601,(1976) , p. 19.
4 申辉旺;邓其源;蔡其巩,未发表资料,1974.
5 陈篪;姚蘅;邓枝生;庄韬;邓其源,金属学报,11(1978) ,174.
6 Mowbray, D. F., Am. Soc. Test. Mater., Spec. Tech. Publ., № 601,(1976) , p. 33.
7 兰州化工机械研究所,未发表资料,1976.
No related articles found!
No Suggested Reading articles found!