Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (5): 571-648    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF Ni ON TEMPERING PROCESS OF MATRIX STEEL
Yu Xuejie; Guo Jiliang; Zhu Jiahua; Huang Jiaping (Shanghai Institute of Iron and Steel Research)
Cite this article: 

Yu Xuejie; Guo Jiliang; Zhu Jiahua; Huang Jiaping (Shanghai Institute of Iron and Steel Research). EFFECT OF Ni ON TEMPERING PROCESS OF MATRIX STEEL. Acta Metall Sin, 1982, 18(5): 571-648.

Download:  PDF(1999KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The tempering behaviour of the matrix steel has been investigated by means of the hardness and strength measurements and TEM observation. It was found that the secondary hardening effect and the resistance to heat softening of the steel are markedly improved by addition of Niabout 1-2%. TEM observation showed that the Ni promotes precipitation of M_2C and transformation of (Fe,M)_3 C as well as fines the grains of V_4C_3 and M_2C. The addition of Ni stabilizes strongly the retained austenite under low temperature tempering. However, the Ni-containing steel tempered under temperature above 500℃ less exceeds Ni-free steel in amount of the retained austenite. The behaviour of increasing the retained austenite does not cover up the effect of strengthening the secondary hardening both by addition of Ni.
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/571

1 肖纪美,高速钢的金属学问题,冶金工业出版社,1976,p.28.
2 #12
3 Speich, G. R., Metall. Trans., 3(1972) , 1043.
4 Porter, L. F.; Manganello, S. J.; Dabkowski, D.S.; Gross, J. H., Met. Eng. Q., 6(1966) , 17.
5 Speich, G. R.; Dabkowski, D. S.; Porter, L. F., Metall. Trans., 4(1973) , 303.
6 Biswas, S. K.; Seal, A. K., Trans. Indian Inst. Met., 21(1968) , №. 4, 21.
7 Chandhok, V. K.; Hirth, J. P.; Dulis, E. J., ASM Trans. Q., 56(1963) , 677.
8 Chandhok, V. K.; Hirth, J. P.; Dulls, E. J., Trans. Metall. Soc. AIME, 224(1962) , 858.
9 Schlatter, R.; Stepanic, J., Met. Progr., 109(1976) , №. 6, 56.
10 Bhat, M. S.; Garrison, W. M., Jr.; Zackay, V. F., Mater. Sci. Eng., 41(1977) , 1.
11 Roberts, G. A.; Hamaker, J. C.; Johuson, A. R., Tool Steels, 3rd Ed., ASM, Metals Park, Ohio, 1962, p. 715.
12 俞学节,金属学报,16(1980) ,53.
13 Daynor, D.; Whiteman, J. A.; Honeycombe, R. W. K., J. Iron Steel Inst., 204(1966) , 349.
14 Heckel, R; Paxton, W., Trans. AIME, 218(1960) , 799.
15 Shimizu, K.; Okamoto, H., Trans. Jpn. Inst. Met., 12(1971) , 273.
No related articles found!