| CALCULATION OF STRESS MEASUREMENT BY X-RAY OSCILLATION METHOD |
| Wang Renzhi (Institute of Aeronautical Materials; Beijing) (Manuscript received 19 January; 1981; revised manuscript 23 May; 1981) |
|
Cite this article:
Wang Renzhi (Institute of Aeronautical Materials; Beijing) (Manuscript received 19 January; 1981; revised manuscript 23 May; 1981). CALCULATION OF STRESS MEASUREMENT BY X-RAY OSCILLATION METHOD. Acta Metall Sin, 1982, 18(4): 493-500.
|
|
|
Abstract For the purpose of the residual stress determination of the materials with coarser grains such as most of Al alloys and Ni-base alloys using X-ray oscillation method, the formulae for the stress calculation have been proposed. It was resulted that the calculated values obtained are fairly consistent with those by conventional X-ray stress measuring methob of fixed ψ_0 angle.
|
|
Received: 18 April 1982
|
1 知久健夫;青山咸恒;并川宏彦;飒田耕三;岩久省吾;多田雅昭,材料,19(1970) , №.207,1028. 2 李仁文,无损检测,(1979) ,№4,40;№5,41. 3 白岩俊男;阪本喜保,X射线应力测定标准方法,附录五,日本材料学会颁发,第一机械工业部机械研究院机电研究所译,1976,p.19.i |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|