| A DISCUSSION ON LONG-RANGE ORDER IN Nb_3 (Al,Ge) COMPOUND WITH A-15 STRUCTURE |
| Jiang Xiaolong Zhang Hong (Shanghai Intitute of Metallurgy; Academia Sinica) (Manuscript received 21 February; 1981) |
|
Cite this article:
Jiang Xiaolong Zhang Hong (Shanghai Intitute of Metallurgy; Academia Sinica) (Manuscript received 21 February; 1981). A DISCUSSION ON LONG-RANGE ORDER IN Nb_3 (Al,Ge) COMPOUND WITH A-15 STRUCTURE. Acta Metall Sin, 1982, 18(4): 439-443.
|
|
|
Abstract A discussion has been made of the possible ordering structure in type A-15 compound Nb_3(Al_(0.75 Ge_(0.25))given previously by Kitchingman et al. The correct X-ray structure factors for several possible ordering structures of this compound are suggested and it is pointed out that the conclusion drawn by Kitchingman etal. seems to be doubtful.
|
|
Received: 18 April 1982
|
1 Arrehenius, G.; Corenzwit, E.; Fitzgerald, R.; Hollo, G.W., Jr., Luo, H.L.; Matthias, B.T.; Zachariasen, W.H., Proc. Nat. Acad. Sci., 61(1968) , 621. 2#12 3 Kitchingman, W. J.; Birch, A., Met. Sci. J., 7(1973) , 191. 4 张宏;姜小龙,物理,11(1982) ,44. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|