THE ELECTROCHEMICAL BEHAVIOUR OF Sb ELECTROWINNING IN Na_2S-NaOH SOLUTION
Jiang Hanying; Shu Yude; Zhao Ruirong; Gong Zhuqing; Yang Songqing (Central South Institute of Mining and Metallurgy; Changsha)
Cite this article: 

Jiang Hanying; Shu Yude; Zhao Ruirong; Gong Zhuqing; Yang Songqing (Central South Institute of Mining and Metallurgy; Changsha). THE ELECTROCHEMICAL BEHAVIOUR OF Sb ELECTROWINNING IN Na_2S-NaOH SOLUTION. Acta Metall Sin, 1982, 18(3): 378-386.

Download:  PDF(707KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By determining the polarization cureve, the discharge potentials of Sb (Ⅲ), Sn (Ⅳ), As (Ⅲ) and H~+ ions were obtain edas -0.92, -1.04, -0.81 and -1.12V respectively, which were checked with the thermodynamic calculation. Their dynamic parameters were estimated by the Tafel lines which resulted after modification of their concentration polarization. At 50℃, the rate constant was found to be 1.54×10~(-4) cm/s, the exchange current density 10~(-2) A/cm~2 and the activation energy 9100 cal/mole.The cathodic discharge mechanism of SbS_3~(3-) and SbS_4~(3-) has been investigated with the help of the chronopotentiometric method. It was shown that before charge transfer, the SbS_3~(3-) ions should be subjected to a prior chemical reaction, i. e. SbS_3~(3-)=SbS~++2S~(2-). The SbS~+ ions formed are then reduced to metallic Sb at the cathode. The discharge of SbS_4~(3-) ions at the cathode takes place in two steps: First, SbS_4~(3-) ions are directly discharged into SbS_3~(3-) and then further reduced into metallic Sb.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/378

1 #12
2 Baibordop, P. P., U. S. S. R. Pat. No. 396 396, 1973. (CA 81:28092c).
3 #12
4 蒋汉瀛;赵瑞荣,中南矿冶学院学报,(1978) ,№.4,66.
5 杨松青;龚竹青,中南矿冶学院学报,(1980) ,№.3,62.
6 舒余德,中南矿冶学院学报,(1980) ,№.3,53.
7 蒋汉瀛,有色金属(冶炼部分)(1981) ,№.2,23.
8 清华大学编,晶体管电路(上册),科学出版社,(1973) .p.394.
9 #12
10 #12
11 #12
12 #12
13 #12
14 物理化学数据简明手册,周振华译(第三版)上海科学出版社,1964,p.100.
15 (1975) , No. 1, 54.
16 #12
17 Delahay, P.; Berzins, T., J. Am. Chem. Soc., 75 (1953) , 2486.
18 查全性,电极过程动力学导论,科学出版社,1976. p.327.
19 Hampel, C. A., The Encyclopedia of Electrochemistry, Chapman & Hall, London, 1964, p. 422.
No related articles found!
No Suggested Reading articles found!