ANALYSIS OF VALENCE ELECTRON AND MAGNETIC MOMENT STRUCTURES OF α-Fe, γ-Fe AND Fe_4N——ELECTRON THEORY OF CASE HARDENING, α-TO γ-Fe PHASE TRANSFORMATION AND CERTAIN OTHER RELATED PROCESSES
Yu Ruihuang (S. H. Yu) (Department of Physics; Jilin University; Changchun; Solid and Molecular Research Group; Jinan University; Guangzhou )
Cite this article: 

Yu Ruihuang (S. H. Yu) (Department of Physics; Jilin University; Changchun; Solid and Molecular Research Group; Jinan University; Guangzhou ). ANALYSIS OF VALENCE ELECTRON AND MAGNETIC MOMENT STRUCTURES OF α-Fe, γ-Fe AND Fe_4N——ELECTRON THEORY OF CASE HARDENING, α-TO γ-Fe PHASE TRANSFORMATION AND CERTAIN OTHER RELATED PROCESSES. Acta Metall Sin, 1982, 18(3): 336-349.

Download:  PDF(1123KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the consideration of series of experimental and theoretical results, the type A and B hybridizations of states of Fe are constructed in the form of 18 discontinuous of hybride levels, belonging to which various valence electrons, atomic magnetic moment and bond length parameters are listed. On the basis of these parameters together with the parameters of N obtained from diatomic molecular spectroscopy, analysis of the valence electron and magnetic moment structures of α-Fe, γ-Fe and Fe_4N=Fe~cNFe_3~f are made. From these structures, interpretation of the space distribution of magnetic moments in the crystalline lattice of α-Fe obtained from neutron diffraction, and interpretation of experimental magnetization curves along [100], [111] and [110] of α-Fe are made and the cause of difference of the atomic magnetic moments of Fe~c and Fef in Fe~cN Fe_3~f are analysed. The phase transformation α-Fe→γ-Fe as due to magnetic origin is contemplated with care. The case hardening by nitriding steel at high temperature and the graphitation in cast iron due to heat effect at high temperature are both traced back to the valence electronic structure origin.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/336

1 余瑞璜(S.H.Yu),科学通报,23(1978) ,217.
2 Mattheiss, L. F., Bull. Am. Phys. Soc., Ser. Ⅱ, 8 (1963) , 222; Phys. Rev., 133 (1964) , A 1399. Seitz, F., The Modern Theory of Solids, McGraw-Hill, New York, 1940, p. 423, Fig. 4.
3 Landolt-Boernstein, I Baund, Atom-und Molekularphysik, 1 Teil, Atome und Ionen, Springer-Verlag, Berlin, 1950, p 60.
4 Mott, N. F.; Jones, H., The Theory of Properties of Metals and Alloys, Oxford Univ. Press, London, 1936, Chapt. 6.
5 Pauling, L., Proc. R. Soc., London, A196 (1949) , 343.
6 王奎雄,王兆民;陈雅符,科学通报、数理化专辑,(1980) ,176.
7 陈雅符;王奎雄;王兆民,科学通报,25(1980) ,974.
8 余瑞璜,科学通报,26(1981) ,206.
9 Hume-Rothery, W.; Raynor, G. V., The Structure of Metals and Alloys, 4th ed., Institute of Metals, London, 1962, p. 198.
10 余瑞璜,Science Reports(暨南大学学报特刊),(1980) ,№1,31.
11 Anderson, J. R.; Gold, A. V., Phys. Rev., 139 (1965) , A 1459.
12 Loucks, T. L., Phys, Rev. Lett., 14 (1965) , 1072.
13 Bizette, H.; Tsai, B., C. R. Hebd. Seances Acad. Sci., 236 (1940) , 252; Bizette, H., J. Phys. Radium, 12 (1951) , 161; Mashiyama, Y.; Uchida, E.; Kendoh, H., Busseiron Ken Kyu (Researches on Chemical Physies), 71 (1954) , 9; Roth, W. L., Phys. Rev., 110 (1958) , 1333; 111 (1958) , 772; Shull, C. G.; Strauser, W. A.; Wollan, E. O., Phys. Rev., 83 (1951) , 333.
14 Teble, R. S.; Graik, D. J., Magnetic Materials, John Wiley, London, 1969 p. 51, Table 2. 16.
15 Abrahams, S. C.; Guttman, L.; Kasper, J. S., Phys. Rev., 127 (1962) , 2052.
16 Bozorth, R. M., Ferromagnetism, D. Van Nostrand Co., Inc., New York, 1953, p. 809.
17 余瑞璜,渗碳体价电子结构分析(待发表)
18 余瑞璜,吉林大学自然科学学报,4(1978) ,54.
19 Thomas, E., J. Sci Instrum., 25 (1948) , 440.
20 Esser, H.; Eusterbrook, H., Arch. Eisenhuettenwes., 14 (1941) , 341; Nid, F. C.; Marnair, D., Phys. Rev., 64 (1941) , 597.
21 Shull, C. G.; Yamada, Y., J. Phys. Soc. Jpn., 17 Suppl. Bill (1962) , 1. Shull, C. G.; Mook, H. A., Phys. Rev. Lett., 16 (1966) , 184.
22 DeCicco, P. D.; Kitz, A., Phys. Rev., 162 (1967) , 486.
23 Frazer, B. C., Phys. Rev., 112 (1958) , 751.
24 Goodenough, J. B., Magnetism and the Chemical Bound, John Wiley & Sons, New York, 1963, p. 342.
25 Jack, K. H., Proc. R. Soc.London, A 195 (1949) , 34.
26 Herzberg, Z., Molecular Spectra of Molecular Structure 1, Spectra of Diatomic Molecules, D. Van Nostrand Co. Inc. Princeton, New York, 1951, p. 243-346, Table 34. , p. 553.
27 Bozorth, R. M., Ferromagnetism, D. Van Nostrand co., Inc., New York, 1953, p. 478.
28 Meyer, A. J. P.; Asch, G., J. Appl. Phys., 32 (1962) , 330.d
No related articles found!
No Suggested Reading articles found!