Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (3): 326-335    DOI:
Current Issue | Archive | Adv Search |
THE DYNAMICAL BEHAVIOUR OF A DISLOCATION GROUP CONTAINING A SOURCE UNDER ALTERNATING LOADING
Patu; Lei Oiongzhi; Ski Changxu (Shih Chang-hsu) (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

Patu; Lei Oiongzhi; Ski Changxu (Shih Chang-hsu) (Institute of Metal Research; Academia Sinica; Shenyang). THE DYNAMICAL BEHAVIOUR OF A DISLOCATION GROUP CONTAINING A SOURCE UNDER ALTERNATING LOADING. Acta Metall Sin, 1982, 18(3): 326-335.

Download:  PDF(764KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The computer simulation method was used to study the dynamical bchaviour of an array of long, straight, parallel coplanar dislocations containing a source under alternating loading which is sinusoidal function of time. It has been found that under alternating loading the glide motion of such a group is irreversible. After each loading cycle, the dislocation group can not recovered to its initial state, and there are ΔN dislocations in the group and the leading dislocation is still at Δx_1 distance from the source. The relation among ΔN, Δx and the loading amplitude, the loading period, the number of loading cycles was also deduced.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/326

1 Eshelby, J. D.; Frank, F. C.; Nabarro, F. R. N., Philos. Mag., 42 (1951) , 351.
2 Cottrell, A. H,, Proc. R. Soc., A285 (1965) , 10.
3 Head, A. K., Philos. Mag., 26 (1972) , 43; 65. Head, A. K., ibid., 27 (1973) , 531.
4 Head, A. K.; Wood, W. W., Philos. Mag., 27 (1973) , 505; 519.
5 Rosenfleld, A. R.; Hahn, G. H., Dislocation Dynamics, Eds. Rosenfleld, A. R.; Hahn, G. H., McGraw-Hill, 1968, p. 255.
6 Kanninen, M. F.; Rosenfleld, A. R., Philos. Mag., 20 (1969) , 569.
7 Rosenfield, A. R.; Kanninen, M. F., Philos. Mag., 22 (1970) , 143.
8 Yokobori, T.; Yokobori, A. T., Jr.; Kamei, A., Philos. Mag., 30 (1974) , 367.
9 Yokobori, A. T., Jr.; Yokobori, T.; Kamei, A., J. Appl. Phys., 46 (1975) , 3720.
10 Atsenault, R. J.; Cadman, T. W., Scr. Metall., 12 (1978) , 633.
11 Arsenault, R. J.; Kuo, C. J. K., Metall. Trans., 9A (1978) , 459.
12 Yokobori, A. T., Jr.; Yokobori, T.; Kamei, A., Mater. Sci. Eng., 40 (1979) , 111.
13 巴图;雷琼芝,金属学报,17(1981) ,177.
14 Patu; Lei, C. Z.; Shih, C. H., Mater. Sci. Eng., 49(1981) ,135.
15 巴图;何怡贞,物理学报,29(1980) ,698. ,
No related articles found!