A NEW MAGNETIC COLLOID TECHNIQUE FOR OBSERVING DOMAIN STRUCTURE OF COATED Si-Fe SHEETS
Luo Yang; Wang Zhenchin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing )
Cite this article: 

Luo Yang; Wang Zhenchin (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing ). A NEW MAGNETIC COLLOID TECHNIQUE FOR OBSERVING DOMAIN STRUCTURE OF COATED Si-Fe SHEETS. Acta Metall Sin, 1982, 18(3): 311-393.

Download:  PDF(2107KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new modified aqueous magnetic colloid was satisfactorily prepared to observe the domain structure of coated Si-Fe sheets. Neither normal field nor other electrical apparatus is necessary for such observation.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/311

1 Yamamoto, T.; Taguchi, S; Sakakura, A; Nozowa, T., IEEE Trans. Magn., MAG-8 (1972) , 677.
2 Holt, C.; Robey, J. A., IEEE Trans. Magn., MAG-5 (1969) , 384.
3 Fathers, D. J.; Jakubovics, J. P.; Jog, D. C.; Newbury, D. E.; Yakowitz, H., Phys. Status Solidi, (a) 20 (1973) , 535.
4 Yamamoto, T.; Nishizawa, H.; Tsuno, K., J. Appl. Phys., 8 (1975) , 79.
5 Mohri, K., Takeuchi, S.; Fujimoto, T., IEEE Trans. Magn., MAG-15 (1979) , 1598.
6 Pfuetzner, H., IEEE Trans. Magn., MAG-17 (1981) , 1245.
7 王振琴,待发表
No related articles found!
No Suggested Reading articles found!