HOT SALT STRESS CORROSION CRACKING OF TITANIUM ALLOY Ti-6A1-4V
Yu Bingxi; Zhang Suisheng and Wan Xiaojing (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

Yu Bingxi; Zhang Suisheng and Wan Xiaojing (Institute of Metal Research; Academia Sinica; Shenyang). HOT SALT STRESS CORROSION CRACKING OF TITANIUM ALLOY Ti-6A1-4V. Acta Metall Sin, 1982, 18(3): 264-271.

Download:  PDF(1831KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Experiments were carried out on the hot salt stress corrosion cracking (HSSCC) of titanium alloy Ti-6Al-4V. The steady-state threshold stress for HSSCC in the temperature range of 300—420℃ was found to be lower than their creep strength at the same temperature. The post-exposure ductility of the specimens after HSSCC is susceptible to the strain rate. By ion microproble analysis, results show that hydrogen is markedly concentrated along the fractographic surface. It seems that the hydrogen produced halide salt corrosion and subsequently absorbed by the titanium alloy is responsible for cracking.
Received:  18 March 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I3/264

1 Petersen, V. C., J. Met., 23 (1971) , No. 4, 40.
2 Ondrejcin, R. S., Metall. Trans., 1 (1970) , 3031,
3 Mahoney, M. W. and Paton, N. E., Corrosion, 28 (1972) , 374.
4 Myers, J. R. and Hall, J. A., ibid., 33 (1977) , 253.
5 Ondrejcin, R. S., NASA CR-1829, 1971.
6 Gray, H. R., Met, Eng. Q., 12 (1972) , No. 4, 10.
7 抚顺钢厂,北京有色金属研究院,未发表资料.
8 Aerospace Structural Metals Handbook, Vol. Ⅱ, 1970, Code 3707, p. 25.
9 万晓景,材料保护,(1979) №.2-3. 11.
10 Gray, H. R., NASA TN D-6188, 1971.
11 Mahoney, M. W. and Tetelman, A. S., Metall. Trans., 7A (1976) , 1549.
No related articles found!
No Suggested Reading articles found!