THE KINETICS OF REACTION BETWEEN Cu_2s-Cu SYSTEM MELTS AND HYDROGEN
Liu Chunpeng;Feng Ganming;Yan Chuanyi;He Aiping Kunming College of Technology; Kunming
Cite this article: 

Liu Chunpeng;Feng Ganming;Yan Chuanyi;He Aiping Kunming College of Technology; Kunming. THE KINETICS OF REACTION BETWEEN Cu_2s-Cu SYSTEM MELTS AND HYDROGEN. Acta Metall Sin, 1982, 18(2): 153-163.

Download:  PDF(742KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  1.The kinetics of reaction between Cu_2S-Cu system melts and H_2 has been studied at 1150,1200,1250 and 1300℃ respectively.Their equations are: for S-rich single phase,u_S=0.717 exp(-(53.137)/(RT))(S%-α)~2p_(H_2)~(1/2)+const. for misc.gap,u_S=0.531 exp(-(67.259)/(RT))p_(H_2)~(1/2) For Cu-rich phase,u_S=44.6 exp(-(146.720)/(RT))p_(H_2)~(1/2)·S%+const. These desulphurization rate are mainly dependent upon the S concentration of melt except the miscible gap.At constant temperature and H_2 partial pressure,their sequence is u_(S(h))>u_(S(m))>u_(S(l)). 2.The mathematic model of desulphurization and activities of S and Cu in relationship to the structure of Cu-S phase diagram are: for S-rich single phase (α=19.81-19.61%S), (?)=A(constant) for miscible gap (b=1.2-19.8%S), (?)=0 for Cu-rich single phase,(0
Received:  18 February 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I2/153

1 Byerley,J.J.;Rempel,G.L.;Takebe,N.,Metall.Trans.,3(1972) ,2133.
2 Byerley,J.J.;Rempel,G.L.;Takebe,N.;Teo,W.K.,Metall.Trans.,4(1973) ,1507.
3 Byerley,J.J.;Rempel,G.L.;Takebe,N.,Metall.Trans.5(1974) ,2501.
4 Ajersch,F.;Toguri,J.M.,Metall.Trans.,3(1972) ,2187.
5 Fukunaka,Y.;Toguri,J.M.,Metall.Trans.,10B(1979) ,191.
6 刘纯鹏,郭有根;艾永衡,金属学报,14(1978) ,373.
7 刘纯鹏,有色金属,1977,№.2,33.
8 吾妻洁;金井勇之进,小川芳树;桥口隆吉,美马源次郎;和田龟吉,金属工学讲座,3,非铁制炼,朝仓书店,1963,p.4,图1. 1.
9 柳桥哲夫等,日本鉱业会志,78(1962) ,43.
10 Schuhmann,R.;Moles,O.W.,Trans.AIME,191(1951) ,235.
11 主编,冶金问题,科学出版社,1960,p.74.
12 Bourgon,M.;Derge,G.;Pound,G.M.,Trans.AIME,209(1957) ,1454.
No related articles found!
No Suggested Reading articles found!