Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (2): 127-140    DOI:
Current Issue | Archive | Adv Search |
SOME ASPECTS OF THE THERMODYNAMICS OF MELTS
Zou Yuanxi;Zhou Jieheng;Xu Yuansen;Zhao Pengnian;Zhang Ziqing Chou Yuanhsi; Shanghai Institute of Metallurgy; Academia Sinica; Institute of Metal Research; Academia Sinica
Cite this article: 

Zou Yuanxi;Zhou Jieheng;Xu Yuansen;Zhao Pengnian;Zhang Ziqing Chou Yuanhsi; Shanghai Institute of Metallurgy; Academia Sinica; Institute of Metal Research; Academia Sinica. SOME ASPECTS OF THE THERMODYNAMICS OF MELTS. Acta Metall Sin, 1982, 18(2): 127-140.

Download:  PDF(1111KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified Gibbs-Duhem equation has been derived with a view to evalu- ating activities of both components of a binary system from the measured ratios of the activities of the two components.This equation has been applied to a num- ber of melts of systems PbCl_2-SnCl_2,PbCl_2-CdCl_2,AgCl-CuCl,Cu_2S-FeS,PbO-BiO_(1.5), PbO-SbO_(1.5),CaO-CaF_2 and CaO-SiO_2-CaF_2 on the basis of our own experimental data as well as those reported in the literature. The method of evaluating activities of Ag and Pb from the binary phase diagram developed a long time ago has been extended to binary systems having a single AB compound.Activities in the In-Sb and Sn-Te systems have been eval- uated in this way. The use of a properly chosen non-ferrous metal instead of Fe as the solvent in the study of slag-metal equilibria with a view to evaluating activities in some ferrous slags has been shown to help in overcoming certain experimental difficul- ties.The systems CaO-SiO_2,CaO-Al_2O_3 and CaO-SiO_2-Al_2O_3 have been investiga- ted by bringing Sn or Cu into equilibrium with the slags.Our recent data on the CaO-SiO_2 system are believed to be sufficiently accurate for the first time to provide a basis for testing the validity of the Masson model.
Received:  18 February 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I2/127

1 王常珍;邹元爔;金属学报,16(1980) ,190.
2 邹元爔;Elliott,J.F.,化学学报,22(1956) ,14.
3 Wagner,C.,Thermodynamic of Alloys,Addison-Wesley,New York,1952,p.19.
4 徐元森;邹元爔;刘辅链,金属学报,7(1964) ,24.
5 徐元森;邹元爔,化学学报,29(1963) ,181.
6 彭瑞伍;陈自姚;邹元爔,金属学报,8(1965) ,401.
7 沈令康;韩兆隆;赵彭年;邹元爔,金属学报,9(1966) ,226.
8 邹元爔,中国科学,13(1964) ,1348.
9 邹元爔,金属学报,6(1963) ,83.
10 Krivsky,W.A.;Schuhmann,R.,Jr.,Trans.AIME,209(1957) ,981.
11 Jel linek,K.,Siewers,H.,Elektrochem.,40(1934) ,871.
12 Strickler,H.S.;Seitz,H.,J.Am.Chem.Soc.,58(1936) ,2084.
13 邹元爔,金属学报,7(1964) ,123.
14 周国治,金属学报,8(1965) ;545.
15 三本木贡治;大谷正康,铁钢,36(1950) ,1.
16 三本木贡治;大谷正康,铁钢,37(1951) ,13.
17 三本木贡洽;大谷正康;中村元,铁钢,38(1952) ,12.
18 Fulton,J.C.;Chipman;J.,Trans.AIME,200(1954) ,1136.
19 Langenberg,F.C.;Chipman,J.;Trans.Metall.Soc.AIME,215(1959) ,958.
20 Philbrook,W.O.;Goldman,K.M.;Helzel,M.M.,Trans.AIME,188(1950) ,361.
21 邹元爔;赵彭年,中国科学,11(1962) ,1287.
22 Kay,D.A.R.;Taylor,J.,Trans.Faraday Soc.,56(1960) ,1372.
23 三本木贡治;大森康男,日本金属学会会志,25(1961) ,139.
24 Elliott,J.F.;Gleiser,M.;Ramakrishna,V.,Thermoehemistry for Steelmaking,Addison-Wesley,New York,1963,Vol.Ⅱ,p.589.
25 Rein,R.H.;Chipman,J.,Trans.Metall.Soc.AIME,233(1965) ,415.
26 沢村企好,铁钢,47(1961) ,1873.
27 Chipman,J.,Trans.Metall.Soc.AIME,221(1961) ,1272.
28 Cowles,A.H.;Cowles,E.H.,U.S.Pat.319 795,424 659,(1884) .
29 Kelley,K.K.,Thermodynamic Properities of Sulfur and Its Inorganic Compounds,U.S.Bureau of Mines,1937,p.406.
30 Kubaschewski,O.;Catterall,J.,Thermoehemical Data of Alloys,Pergaman,New York,1956,p.151.
31 Ruddle,R.W.,The Physical Chemistry of Copper Smelting,IMM,London,1953,p.106.
32 Barker,I.L.;Jacobi,J.S.;Wadis,B.H.,Trans.AIME,209(1957) ,774.
33 Lumsden,J.,Metallurgical Society Conferences,Intersciences Publishers,New York,Vol.7,1961,p.165.
34 Terpilowski,J.,Arch.Burn.,4(1959) ,355.
35 #12
36 Masson,C.R.,J.Iron Steel Inst.,210(1972) ,89.
37 Darken,L.S.,Thermodynamics in Physical Metallurgy,ASM,Cleveland,1950,p.28.
38 Fetters,K.L.;Chipman,J.,Trans.AIME,145(1941) ,95.
39 Taylor,C.R.;Chipman,J.,Trans.AIME,154(1943) ,228.F
No related articles found!