Acta Metall Sin  1982, Vol. 18 Issue (2): 115-126    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMICS ON THE SELECTIVE OXIDATION OF ELEMENTS IN MOLTEN MATTE AND METALS
Wei Shoukun Beijing University of Iron and Steel Technology
Cite this article: 

Wei Shoukun Beijing University of Iron and Steel Technology. THERMODYNAMICS ON THE SELECTIVE OXIDATION OF ELEMENTS IN MOLTEN MATTE AND METALS. Acta Metall Sin, 1982, 18(2): 115-126.

Download:  PDF(958KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The selective oxidation of elements in molten matte and metals is reviewed and discussed from thermodynamic viewpoint,Ni vs S in nickel matte,Cr,V,Nb, Mn or P vs C in iron melts being taken as examples of practical application.On grounds of thermodynamical analysis,a concept of transition temperature of oxi- dation has been introduced,and methods of calculating the transition temperature with either the two-steps- or the one-step-method are presented.On the assumption that no nucleation energy is required for the formation of new phases (gas bub- bles and the condensed oxidation products),the transition temperature of oxida- tion is independent of the forms of oxygen present,be it gaseous oxygen,dissolved [O] in metal melts or FeO from the slag,and also independent of the pressure or activity of oxygen,but it depends solely upon the nature and activity (pressure) of the reactants and products taking part in the reaction.Furthermore,the transi- tion temperature of oxidation is not a fixed temperature,it varies continuously with the composition of the bath as the oxidation process goes on.Reducing the pressure of the gaseous product would help to lower the transition temperature of oxidation. With the transition temperature of oxidation theoretically calculated,it is possible to deduce the optimal conditions for allowing one element preferentially oxidized while leaving the other element practically intact in the bath.Small- scale experiments and industrial practices show that the concept of the transition temperature of oxidation does successfully serve as a guide to control the blowing (smelting) operation,with the result that the desired element could be oxidized selectively.The kinetic factors which influence the sequence of oxidation of ele- ments in the bath are also briefly discussed. For the desulphurization of nickel matte,the decarburization in the 18-9 stainless steel manufacture (including the AOD process)and the decarburization of high-carbon ferromanganese,the blowing operation should be run so that the temperature of the bath should always be higher than the transition temperature of oxidation corresponding with the composition of the bath.But for the dechro- mizing of pig iron,and the extraction of V or Nb from the pig iron,smelting operation should be carried on,so that the temperature of the bath should be kept always lower than the transition temperature of oxidation for the respective com- position of the bath.As regards the sequence of oxidation of P with respect to C,besides the effect of the transition temperature of oxidation,the basicity and the FeO-content of the slag for holding P_2O_5 as well as the pressure exposed to or sustained by the CO-bubbles should be both considered.
Received:  18 February 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I2/115

1 Bodsworth,C.;Bell,H.B.,Physical Chemistry of Iron and,Steel Manufacture,2nd,Longman,London,1972,p.198.
2 Bodsworth,C.;Bell,H.B.,ibid.,p.203.
3 Sigworth,G.K.;Elliott,J.F.,Met.Sci.,8(1974) ,298;Elliott,J.F.,Electr.Furnace Proc.,32(1974) ,62.
4 Elliott,J.F.;Gleiser,M.Q.;Ramakrishna,V.,Thermochemistry for Steelmaking,Vol.Ⅱ,AddisonWesley,New York,1963,p.620.
5 韩其勇,个人通讯,1973;转炉氧气斜吹硫化镍探索性试验总结,(内部资料).1971.
6 魏寿昆,回转炉氧气吹炼冰镍的物理化学,1973(未发表论文).
7 魏寿昆,冶金过程热力学,上海科技出版社,1980,p.103.
8 魏寿昆;洪彦若,镍锍选择性氧化的热力学及动力学,1980年广州冶金过程物理化学学术报告会论文;有色金属33(1981) ,№3,50.
9 北京钢铁学院冶金物化专业,72年级冶炼学习汇报材料汇编,1975,p.5-9.
10 Schenck,H.;Wenzel,W.;Joshyula,G.K.M.,Arch.Eisenhuettenwes.,34(1963) ,503.
11 林宗彩;周荣章,钢铁,14(1979) ,№.3,1.
12 文献[7] ,p.70;1. 5吨摇包脱铬补充试验(内部资料),1978.
13 文献[7] ,p.71.
14 Sims,C.E.,Electric Furnace Steelmaking,Vol.Ⅱ,Interscience,New York,1963,p.172.
15 魏寿昆,冶炼过程热力学(内部讲义),1974 p.2-22;文献[7] ,p.76.
16 魏寿昆,炼钢冶金原理,(内部讲义),1977. p.2-88;文献[7] p.86.
17 魏寿昆,含钒铁水炼钢的一些物理化学问题,攀钢技术处(内部资料)1976;文献[7] ,p.87.
18 文献[16] ,p.2-100;文献[7] ,p.29.
19 文献[16] ,p.2-99;文献[7] ,p.90.
20 林宗彩;周荣章等,北京钢铁学院学报,1980,№.2,p.25.
21 张庆宜,钢铁,15(1980) ,№.8,13.
22 邵象华,金属学报,13(1977) ,182.
23 魏寿昆,金属学报,7(1964) ,240.
24 文献[16] ,p.4-95;文献[7] ,p.280.
25 Rellermeyer,H.;Knuepple,H.;Sittard,J.,Stahl Eisen,77(1957) ,1296.x
No related articles found!
No Suggested Reading articles found!