Acta Metall Sin  1982, Vol. 18 Issue (1): 85-134    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF Cr ON "SOFTENING EFFECT" OF 30CrNiSMoV STEEL
Lu Zaojun; Wu Baorong; Wu Peizhi; Li Guiyen; Wang Qi; Lu Hongxiu; Li Xueyuan; Jin Qingqian; Wang Degen (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
Cite this article: 

Lu Zaojun; Wu Baorong; Wu Peizhi; Li Guiyen; Wang Qi; Lu Hongxiu; Li Xueyuan; Jin Qingqian; Wang Degen (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). INFLUENCE OF Cr ON "SOFTENING EFFECT" OF 30CrNiSMoV STEEL. Acta Metall Sin, 1982, 18(1): 85-134.

Download:  PDF(1472KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of Cr contents on the softening effect of steel 30CrNi5MoV was investigated by using optical microscopy, TEM and phase analysis. The conditional proportion limit, σ_p_(50), of the steel falls sharply as the increasing of Cr contents in the range 0.22—1.61% under same other experimental conditions. It was deduced that its falling rate is expressed as: σ_p_(50)=1352—245×Cr%. The softening effect may be substantially resulted from that Cr changes the solubility of solute in α-ferrite, coarsens the martensitic substructure and reduces the ratio of the grain size of carbides to their interparticle spacings.
Received:  18 January 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I1/85

1 Lacy, C. E.; Gensamer, M., Trans. ASM, 32 (1944) , 88.
2 Leslie, W. C.; Sober, R. J.; Babcock, S. G.; Green, S. J., ASM Trans. Q., 62 (1969) , 691.
3 Leslie, W. C., Metall. Trans., 3 (1972) , 5.
4 Tanaka, T.; Watanabe, S., Acta Metall., 19 (1971) , 991.
5 Ulitchny, M. G.; Vasndevan, A. K.; Gibala, R., The Microstructure and Design of Alloys, Proc. 3rd Int. Conf. on the Strength of Metals and Alloys, Vol. 1, Cambridge, England, 1973, p. 505.
6 Spitzig, W. A.; Leslie, W. C., Acta Metall., 19 (1971) , 1143.
7 Spitzig, W. A., Mater. Sci. Eng., 16 (1974) , 169.
8 Kelley, M. J.; Stoloff, N. S., Metall. Trans., 7A (1976) , 331.
9 Thomas. G., Iron Steel Int., 46 (1973) . 451.
10 小林泽;白沢秀则;自在丸二郎,铁钢,66(1980) ,685.
11 Ansell,G.S.未发表资料;1979.
12 Bush, M. E.; Kelly, P. M., Acta Metall., 19 (1971) , 1363.
13 Bergstroem, Y.; Josefsson, ■., Scan. J. Metall., 3 (1974) , 259.
14 Norstroem, L.-■., Scan, J. Metall., 5 (1976) , 41.
15 Smith, D. W.; Hehemarm, R. F., J. Iron Steel Inst., 209 (1971) , 476.
16 Naylor, J. P., Metall. Trans., 10A (1979) , 861.
17 Irvine, K. J.; Pickering, F. B., J. Iron Steel Inst., 201 (1963) , 944.L
No related articles found!
No Suggested Reading articles found!