Abstract A study was made on the microstrueture, properties and deformation behaviour of intercritically quenched ferrite-martensite dual-phase steel 20 under coldrolling. The results indicate that both structure and properties of martensite and ferrite phases are quite different from those of single-phase ones. The conventional mixture law, which is commonly used to evaluate the strength of the fibre-reinforced composite materials seems to be not applicable. The model of deformation of the dual phase steel 20 in the process of cold rolling may be proposed by a gradual transition from stress-equal model at the starting to strain-ratio-equal model on the later stage. Its work-hardening may be attributed to a change from nonequal strengthening state to strength-ratio-equal state A summarized plot for its deformation behaviour during cold-rolling is also given to understand rather easily the relative variation of the structure and properties of each phase in the whole process.
|
|
Received: 18 January 1982
|
1 Rashid, M. S., SAE Technical Paper, Preprint 760 206, 1976. 2 Davies, R. G.; Magee, C. L., J. Met. 31 (1979) , No 11, 17. 3 Kot, R. A.; Morris, J. W., Structure and Properties of Dual Phase Steels, Proc. AIME Symp. at Annual Meeting in New Orleans, Feb. 1979. 4 Thorton, P. H.; Metall Trans., 10 (1979) , 1179. 5 Bailey, D. J.; Stevenson, R., ibid., 47. 6 Davies, R. G., ibid., 113. 7 Davies, R. G., ibid., 9A (1978) , 671. 8 Ramos, L. F.; Matlock, D. K.; Krauss, G., Metall. Trans., 10A (1979) , 259. 9 田村今男;友田阳;山岡幸男;金谷三郎;小沢正俊;赤尾明,铁钢,59(1973) ,454. 10 Koo, J. Y.; Young, M. J.; Thomas, G., Metall, Trans., 11A (1980) , 852. 11 Mileiko, S. T., J. Mater. Sci., 4 (1969) , 974. 12 Metals Handbook, ASM, Vol. 1, 1961, p. 1234. 13 友田阳;黑木刚司郎;田村今男,铁钢,61(1975) ,107. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|