Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (1): 11-118    DOI:
Current Issue | Archive | Adv Search |
THE MECHANISM OF NON-EQUILIBRIUM SEGREGATION OF BORON TO AUSTENITE GRAIN BOUNDARIES
He Xinlai; Chu Youyi; Ke Jun (T. Ko) (Beijing University of Iron and Steel Technology; Beijing)
Cite this article: 

He Xinlai; Chu Youyi; Ke Jun (T. Ko) (Beijing University of Iron and Steel Technology; Beijing). THE MECHANISM OF NON-EQUILIBRIUM SEGREGATION OF BORON TO AUSTENITE GRAIN BOUNDARIES. Acta Metall Sin, 1982, 18(1): 11-118.

Download:  PDF(8827KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It has been demonstrated that the boron segregation at austenite grain boundaries in quenched steel is a non-equilibrium grain boundary segregation phenomena occurred during cooling. In this paper, by way of resolving nonisothermal diffusion equation, a theoretical formula for non-equilibrium grain boundary segregation has been derived, and the relationship among width of boron depleted zone, quenching temperature, cooling rate, activation energy and diffusion constant of non-equilibrium grain boundary segregation has been established. The theoretical prospects agreed with experimental results satisfactorily.From experimental results and theoretical analysis, an atomic model for nonequilibrium grain boundary segregation has been suggested, based on the moving of boron atoms along with supersaturationies vacancies or divacancies to grain boundaries (sink of vacancy) during cooling. In light of this new idea of nonequilibrium grain boundary segregation, the complicated effects of boron on hardenability of steel can be explained unambiguously.
Received:  18 January 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I1/11

1 贺信莱;褚幼义;柯俊,金属学报,18(1982) ,1.
2 Crank, J., The Mathematics of Diffusion, Oxfold, Clarendon Press, 1975.
3 淬火介质,白云昭译,机械工业出版社,1965,p.1-13.
4 Hanncman, R. E.; Anthony, T. R., Acta Metall., 17 (1969) , 1133.
5 Aust, K. T.; Hanneman, R. E.; Niesscn, P.; Westbrook, J. H., Acta Metall., 16 (1968) , 291.
6 Bercovici, S. J.; Hunt, C. E. L.; Nicssen, P., J. Mater. Sci.,5 (1970) , 326.
7 Watanabe, T.; Kitamura, S.; Karashima, S., Acta Metall., 28 (1980) , 455.
8 Williams, T. M.; Stoncham, A. M.; Harrics, D. R., Met. Sci., 10 (1976) , 14.
9 Balluiffi, R. W.; Lie, K. H.; Seidman, D. N., Vacancies and Intcrstitials in Metals, Ed. Seeger, A.; North-Holland, 1970.
10 Smith, A. F.; Gibbs, G. B., Metal Sci. J., 2 (1968) , 47.
11 Flynn, C. P., Point Dcfccts and Diffusion, 1972, Clarendon Press, Oxford, p. 788.
12 Hudson, J. A.; Nelson, R. S., Vacancies "76", Eds. Smallman, R. E.; Harris, J. E., 1977, p. 126.
13 Busby, P. E.; Warga, M. E.; Wells, C., J. Met., 5(1953) , 1463.
14 Simeoe, C. R.; Elsea, A. R.; Manning, G. K., Trans. AIME, 203 (1955) , 193; 206 (1956) , 984.
15 贺信莱,褚幼义等,待发表.N
No related articles found!
No Suggested Reading articles found!