| ON THE LONGITUDINAL CRACKS IN 30CrMnSiNi2A ELECTROSLAG INGOT |
| by Jiang Jinwen (Institute of № 1 Steel works; Benxi Iron and Steel Company); Liu Xingzhi and Tian Jifeng (Institute of Metal Research; Academia Sinica) |
|
Cite this article:
by Jiang Jinwen (Institute of № 1 Steel works; Benxi Iron and Steel Company); Liu Xingzhi and Tian Jifeng (Institute of Metal Research; Academia Sinica). ON THE LONGITUDINAL CRACKS IN 30CrMnSiNi2A ELECTROSLAG INGOT. Acta Metall Sin, 1981, 17(5): 549-608.
|
|
|
Abstract The cause and remedy of the longitudinal cracking in 30CrMnSiNi2A electroslag ingot have been investigated. Results showed that the cracks are initiated by the microsegregated C, P, S, Si, etc. along the primary austenite boundaries which become fragile and cracking under higher thermal stress. Al is injurious owing to promoting the microsegregation of elements and brittle fracture of grain boundaries rather than formation of the AlN. An effectual remedy for longitudinal cracks in 30CrMnSiNi2A electroslag ingot is to keep the residual amount of Al under control if the heat-retaining condition is restricted after stripping the ingot.
|
|
Received: 18 May 1981
|
[1] Desai, S. C., J. Iron Steel Inst., 191 (1959) , 250. [2] Biggs, B. L., J. Iron Steel Inst., 192 (1959) , 361. [3] Ericson, L., Scand. J. Metall., 6 (1977) , 116. [4] Irvine, K. J. and Pickering, F. B., Iron Steel, 30 (1957) , 219. [5] #12 [6] #12 [7] Kajioka, H., Yamaguchi, K., Sato, N., Soejima, K. and Sakaguchi, S., Proc. of the Fourth Int. Symp. on Electroslag Remelting Processes, Tokyo, ISIJ, 1973. [8] 氏家信久,日本金属学会会报,5(1966) ,№ 1,17. [9] Erasmus, L. A., J. Iron Steel Inst. 202 (1964) , 32. [10] Woodfine, B. C. and Quarrell, A. G., J. Iron Steel Inst., 195 (1960) , 409. [11] Pokorny, A. J., De Ferri Metallographia Ⅲ, Berger-Levrant, 1967, p. 47. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|