PRELIMINARY STUDIES ON KINETICS OF HIGH PRESSURE HYDROGEN REDUCTION OF NICKEL ION IN AQUEOUS SOLUTION TO METALLIC NICKEL
by Shu Daixuan; Mao Minghua and Chen Jiayong (Institute of Chemical Metallurgy; Academia Sinica)
Cite this article: 

by Shu Daixuan; Mao Minghua and Chen Jiayong (Institute of Chemical Metallurgy; Academia Sinica). PRELIMINARY STUDIES ON KINETICS OF HIGH PRESSURE HYDROGEN REDUCTION OF NICKEL ION IN AQUEOUS SOLUTION TO METALLIC NICKEL. Acta Metall Sin, 1981, 17(4): 403-411.

Download:  PDF(608KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies were made on high pressure hydrogen reduction of Ni ammoniacal solution to metallic Ni with fine Ni powder, which was also prepared by hydrogen reduction with Cr~(2+) as nucleating agent, added as solid seed. Results indicate that the reduction was carried out under chemical reaction rate control region. The rate of reduction is proportional to the amount of Ni powder as solid seed added,and to the square root of partial pressure of hydrogen and is not influenced by the concentration of Ni ion in solution up to most of Ni reduced. Both activation of hydrogen molecules and phase transformation of Ni are believed to proceed on the surface of Ni powder added. Reaction can be considered to proceed according to the following scheme with reaction 4 as the rate controlling step:(5) 2H~++2NH_3=2NH_4~+ fast
Received:  18 April 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I4/403

[1] Evans, D. I. J., Advances in Extractive Metallurgy, IMM, London, 1968, p. 831.
[2] Burkin, A. R. and Richardson, F. D., Powder Metall., 10 (1967) , 33.
[3] Derry, R., Miner. Sci. Eng., 4 (1972) , No. 4, 3.
[4] Schaufelberger, F. A., J. Met., 8(1956) , 695.
[5] 舒代萱,毛铭华,陈家镛,全国第一届冶金过程物理化学学术报告会论文集,1965,上海科学技术出版社,p.107.
[6] Knacke, O., Pawlek, F. and Sussmuth, E., Z. Erzbergbau Metall. 9 (1956) , No. 12, 566.
[7] Sircar, S. C. and Wiles, D. R., Trans. Metall. Soc. AIME, 218 (1960) , 891.
[8] Mackiw, V. A., Lin, W. C. and Kunda, W., Trans. Metall. Soc., AIME, 209 (1957) , 786.
[9] #12
[10] Needes, C. R. S. and Burkin, A. R., Leaching and Reduction in Hydrometallurgy, Ed. by A. R. Burkin Inst. Min. Metall., London, 1975, p, 91.
[11] 坂野武,永野健,寺田富士朗,日本矿冶会誌,75(1959) ,853.
No related articles found!
No Suggested Reading articles found!