Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (3): 359-361    DOI:
Current Issue | Archive | Adv Search |
DETERMINATION OF SURFACE TENSION AND ITS TEMPERATURE COEFFICIENT OF MOLTEN URANIUM
by Wang Jingtang; Bian Maoshou and Zeng Mengcang (Institute of Metal Research; Academia Sinica)
Cite this article: 

by Wang Jingtang; Bian Maoshou and Zeng Mengcang (Institute of Metal Research; Academia Sinica). DETERMINATION OF SURFACE TENSION AND ITS TEMPERATURE COEFFICIENT OF MOLTEN URANIUM. Acta Metall Sin, 1981, 17(3): 359-361.

Download:  PDF(176KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 March 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I3/359

[1] Rosen, C. L., Chellew, N. R., and Feder. H. M., Nucl. Sci. Eng., 6 (1959) , 504.
[2] Spriet, B., Mem. Sci. Revu. Met., 60 (1963) , 531.
[3] Cahill, J. A., Kirshenbaum, A. D., J. Inorg. Nucl. Chem., 27 (1965) , 73.
[4] Hoage, J. H., HW-78132 (1963) .
[5] Grosse, A. V., Cahill, J. A. and Kirshenaum, A. D., J. Amer. Chem. Soc., 83 (1961) , 4665.
No related articles found!