| STRUCTURAL AND MAGNETIC PROPERTIES OF Y (Mn_(1—x)Fe_x)_(12) |
| by Yang Yingchang (Dept. of Physics; Beijing University) |
|
Cite this article:
by Yang Yingchang (Dept. of Physics; Beijing University). STRUCTURAL AND MAGNETIC PROPERTIES OF Y (Mn_(1—x)Fe_x)_(12). Acta Metall Sin, 1981, 17(3): 355-358.
|
|
|
Abstract The new ternary intermetallic compounds on the iron rich side Y(Mn_(1-x)Fe_x)_(12) have been prepared and their magnetic properties investigated. Their structure was found to be of the ThMn_(12) type with x=0.8 after appropriate annealing. The field dependence of magnetization was measured under range of 4.2 K to room temperature. The results indicate that Y(Mn_(1-x)Fe_x)_(12) appears antiferromagnetic when x=0.0, 0.2 or 0.4, in a spontaneous magnetization when x=0.6 and to become ferromagnetic or ferrimagnetic when x=0.8. The Curie point is above room temperature.
|
|
Received: 18 March 1981
|
| [1] Deportes, J., Givord, D., Lemaire, R. and Nagai, H., Physica, 86-88B (1977) , 69-70 (c). |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|