RECENT PROGRESS IN HVEM AND ITS APPLI-CATIONS TO THE STUDY OF PROPERTIES OF METALLIC MATERIALS
Taoka Tadami (Institute of Vocational Training; Sagamihara; Kanagawa; Japan)
Cite this article: 

Taoka Tadami (Institute of Vocational Training; Sagamihara; Kanagawa; Japan). RECENT PROGRESS IN HVEM AND ITS APPLI-CATIONS TO THE STUDY OF PROPERTIES OF METALLIC MATERIALS. Acta Metall Sin, 1981, 17(3): 307-351.

Download:  PDF(15499KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Ⅰ. IntroductionⅡ. Advantages of HVEM2.1 Enhancement of resolution for thicker specimen2.2 Improvement of penetrating power2.3 Broadening the scope of thicker specimen observation2.4 Improvement of visibility and contrast of crystal defects and dislocation image2.5 Accuracy of selected area diffraction2.6 Irradiation damge, bombardment damage in metals and ionization damage in organic substances2.7 Critical voltage effects2.8 Special imaging techniques to improve contrastr in HVEM2.9 High voltage scanning transmission electron microscope2.10 In-situ observation of dynamic processⅢ.Specimen, its treatment and observation conditions 3.1 Specimen3.2 Orientation control of specimen3.3 Condition of specimen treatingⅣ. Identification of crystal defects and their fundamental properties4.1 Point defects and their migration4.2 Dislocation4.3 Dislocation loop4.4 Stacking fault4.5 Small angle grain boundary and coincidence grain boundary4.6 precipitates and inclusionⅤ.Relationship between microdtructure and macro-properties5.1 Mechanical properties5.2 Recovery and recrystallization5.3 Phase transformation, nucleation and growth of precipitates5.4 Magnetic domain, structure of domain wall and its temperature dependence5.5 Property of semiconducting grains and crystal defects5.6 Electron irradiation damage5.7 Application of critical voltage effect to the study of material properties5.8 Illustration of in-situ observation Concluding remarks
Received:  18 March 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I3/307

[1] HVEM応用関综合報告
1) Franks, A. and Halliday, J. S., Engineering, 192 (1961) , 94.
2) 上田良二,榊米一郎,科学,36(1966) ,114.
3) 藤田広志,日本金属学会会報,5(1966) ,85.
4) Cosslett, V. E., Phys Today, 21 (1968) , № 7, 23.
5) Hashimoto, H. JEOL Rep. on Application of Electron Microscopy, 1968, p. 23.
6) 井村徹,物性,(1969) ,567.
7) Taoka, T., Proc. 3rd Int. Symposium, (1960) at Dresden, DDR, 'Einstoffe in Wissenshalt und Technik', p. 589.
8) 田岡忠美,铁鋼,59(1973) ,988.
9) Dupouy, G., Proc. 4th Int. Conf. HVEM at Toulouse (1975) , 'microscopic electronique a haute tension', p. 1.
10) 藤田広志,電子顕微鏡,12(1977) ,2.
11) 井村徹,電子顕微鏡,12(1977) .7.
12) Hirsch, P. B., Proc, 5th Int. Conf. HVEM, at. Kyoto (1977) , 'High Voltage Electron Microscopy', p. 21.
[2] Thomas, G., Proc. 9th Int. Cong. EM, at Tronto (1978) , 'Electron Microscopy', Vol. 3, p. 392.
[3] Hashimoto, H., Tanaka, K., Kobayashi, K., Suito, E., Shimadzu, S. and Iwanaga, M., Proc. Int. Conf. on Magnetism and Crystallography, at Kyoto (1961) , Vol. Ⅱ, 'Electron and Neutron Diffraction', p. 170. Hashimoto, H., J. Appl. Phys., 35 (1964) , 277.
[4] Hirsch, P. B., Proc. Int. Conf. on Magnetism and Crystallography at Kyoto (1961) , J. Phys. Soc. Jap., 17 (1962) Suppl. B-Ⅱ, 143.
[5] Fujita, H., Kawasaki, Y., Furubayashi, E., Kajiwara, S. and Taoka, T., Jap. J. Appl. Phys., 6 (1967) , 214.
[6] Kamiya, Y., J. Phys. Soc. Jap., 27 (1969) , 956.
[7] Ploc, R. A., Rcp. of Atomic Energy of Canada Ltd., AECL-3904 1971, p. 1.
[8] Uyeda, R. and Nonoyama, M., Jap. J. Appl. Phys., 6 (1967) , 557. Uyeda, R. and Nonoyama, M., ibid., 7 (1968) , 200.
[9] Thomas, G., Phil. Mag., 17 (1968) , 1097.
[10] Fujita, H., Tabata, T., Yoshide, K., Sumida, N. and Katagiri, S., Jap. J. Appl. Phys., 11 (1972) , 1522.
[11] Watanabe, H., Fukuhara, A. and Kora, K., Proc. Int. Conf. Magnetism and Crystallography (1961) at Kyoto, J. Phys. Soc. Jap., 17 (1962) , Suppl. B-Ⅱ, 195. Uyeda, R., ibid., 155. 神谷芳弘,J. Electron Microscopy, 19 (1970) , 245.
[12] Fujiwara, K., J. Phys. Soc. Jap., 16 (1961) , 2226.
[13] JEOL., JEM, 1000/1250.
[14] Hirsch, P. B., Howic, A., Nicholson, R. B., Pashley, D. W. and Whelan, M. J., Electron Microscopy of Thin Crystals, Butterworths, 1965, p. 496.
[15] Hashimoto, H., Howie, A. and Whelan, M. J., Phil. Mag., 5 (1960) , 967, Table A4. 2 Hashimoto, H., Howie, A. and Whelan, M. J., Proc. Roy. Soc. A 269 (1962) , 80.
[16] Humphreys, C. J., Thomas, L. E., Lally, J. S. and Fisher, R. M., Phil. Mag., 23 (1971) , 87.
[17] Humphrevs. C. J., Proc. 25th Annivcrsarv Meet. EMAG. INST. Physics. 1971. p. 12.
[18] 古林英一,铁鋼,58(1972) ,343.
[19] Hashimoto, H., Pnoc. 5th Int. Cong. EM at Philadelphia (1962) B, p. 11. Hashimoto, H., Rcp. of JEOL (1968) , 'Application of Electron Microscopy', Part Ⅱ, p. 23.
[20] Uyeda, R., Dupouy, G., Perrier, F., Ayroles, R.,and Bousguet, A., J. Eiectronmicrroscopy, 12 (1963) , 271.
[21] Ino, S., Ogawa, S., Taoka, T. and Akahori, H., Jap. J. Appl. Phys., 11 (1972) , 1859.
[22] Makin, M. J., Phil. Mag., 18 (1968) , 637. Markin, M. J., Proc. 9th Int. Cong. EM at Tronto (1978) , 'Electron Microscopy', Vol. Ⅲ, p. 330.
[23] Kiritani, M. and Yoshida, N., J. Phys. Soc. Jap. 36 (1974) , 613. Kiritani, M., Yoshida, N., Takata, H. and Maehara, Y., J. Phys. Soc. Jap. 38 (1975) , 1677. 桐谷道雄,吉田直亮,電子顕微鏡,10(1975) ,97. 桐谷道雄,日本金属学会報,17(1978) .646.
[24] Doran, D. G., Nucl. Eng. Design, 33 (1975) , 63.
[25] 竹山大郎,日本金属学会報,13(1974) ,591. 竹山大郎,電子顕微鏡,11(1976) ,21.
[26] Glacser, R. M., Proc. 3rd Int. Conf. HVEM at Oxford (1974) , p. 370.
[27] 渡辺伝郎,福原明,日本结晶学会誌,10(1968) ,255. 渡辺伝郎,日本金属学会報,14(1975) .481.
[28] Nagata, F. and Fukuhara, A., Jap. J. Appl. Phys., 6 (1967) , 1233. Fukuhara, A. and Yanagisawa, A., Jap. J. Appl. Phys., 8(1969) , 1166.
[29] Uyeda, R., Acta Cryst., A24 (1968) , 175. Watanabe, D., Uyeda, R. and Fukuhara, A., ibid, 580.
[30] Goringe, M. J., Proc. 4th Int. Conf. HVEM at Toulouse (1975) , 'microscopic electronique a haute tension', p. 85.
[31] Bell, W. L, Proc. Workshop Conf, on Microscopy of Cluster Nuclei in Defected Crystals at Chalk River, (1971) , p. 111. Butler, E. P., Proc. 3rd Conf. HVEM at Oxford (1973) , 'High Voltage Electron Microscopy', p. 22.
[32] Osiecki, R. and Thomas, G., 29th Ann. Proc. of EMSA at Boston (1971) , p. 178.
[33] Hashimoto, H., Proc. 2nd Int. Conf. HVEM at Stockholm (1971) , Jern. Ann. 155 (1971) , 479.
[34] Yamamoto, T., Nishizawa, H., Uchida, U., Shibatomi, K. and Taoka, T., JEOL News, 10e (1972) , № 3, 10.
[35] Cockayne, D. J. H., Ray, I. L, F. and Whelan, M. J., Phil. Mag. 20 (1969) , 1265.
[36] Crew, A. V., Proc. 9th Int. Cong. EM at Tronto (1978) , 'Electron Microscopy', 1978, Vol. Ⅲ, p. 197. 小池紘民,日本電子顕微鏡学会報,1,73,№ 6,82.
[37] Zeitler, E. and Crew, A. V., Proc. 5th Int. Conf. HVEM at Kyoto (1977) , p. 99.
[38] Strojinik, A., Cosslett, V. E. and Sparrow, T. G., Proc. 5th Int. Conf. HVEM at Kyoto (1977) , p. 103.
[39] Coeley, I. M., Appl. Phys. Lett., 15 (1969) , 58.
[40] Yamamoto, T., Nishizawa, H. and Shibatomi, K., Proc. 8th Int. Cong. EM at Canberra, (1974) , Electron Microscopy, Vol. 1, p. 286. Yamamoto, T. and Nishizawa, H., JEOL News, 12e (1974) , № 2, p. 19.
[41] Crew, A. V. and Wall, J., Optik, 30 (1970) , 461. Cowley, J. M., Proc. 5th Int. Conf. HVEM at Kyoto (1977) , 'High Voltage Electron Microscopy', p. 9.
[42] Ishikawa, A. Morita, C., Hibino, M. and Maruse, S., Proc. 5th Int. Conf. HVEM at Kyoto (1977) , 'High Voltage Electron Microscopy', p. 105.
[43] Yamamoto, T., Tsuno, K. and Nishizawa, H., Proc. 33rd Ann. EMSA. at Las Vegas (1975) , p. 32. Yamamoto, T., Nishizawa, H. and Tsuno, K., J. Phys. D: Appl. Phys., 8 (1975) , L 113.
[44] 井村徹,藤田広志,電子顕微鏡,10(1975) ,59.
[45] 井村徹,日本物理学会誌,25(1970) ,815.
[46] Hirsch, P. B., Howie, A., Nicholson, R. B., Pashley, D. W. and Wehlan, M. J., 'Electron Microscopy of Thin Crystals', Butterworths,1965. p.24. ;西山善次,幸田成康编,金属電子顕微镜写真解說,丸善KK,1974,p.321.
[47] Imura, T., Proc. 3rd Int. Conf. HVEM at Oxford (1973) , 'High Voltage Electron Microscohy', 1973, p. 179.
[48] Wakashima, K., Fukamachi, M. and Nagakura, S., Jap. J. Appl. Phys., 8 (1969) , 1167. Wakashima, K., Nagakura, S. and Taoka, T., Acta Met., 20 (1972) 133.
[49] Taukahara, S., Kawakatsu, H. and Taoka, T., Proc. 2nd Int. Conf. HVEM at Stockholm,(1971) , Jern. Ann., 155 (1971) , 468.
[50] Uchida, Y., Lehmpfull, G. and Fujimoto, F., Proc. 5ht Int. Conf. HVEM at Toulouse (1975) ,'microscopic electronque, a haute tension', 1975, p. 113.
[51] JEOL. Technical Rep. (柴富氏提供)
[52] JEOL. Technical Rep. (柴富氏提供)
[53] 深見章,村上悟,電子顕微鏡,9(1974) ,4. Fukami, A. and Murakami, S., Proc. 30th Annie. Jap. Soc. EM at Takarazuka (1979) , J. Electron microscopy. 28 (1979) , Suppl., s41.
[54] Swann, P. R., Proc. 4th Int. Conf. HVEM at Toulouse (1975) , 'microscopic electronique a haute tension', 1975, p. 299. Swann, P. R., Proc. 9th Int. Cong. EM at Tronto (1978) , 'Electron Microscopy', 1978, Vol. Ⅲ, p. 319.
[55] Sakata, S. and Tanino, M., Proc. 5th Int. Conf. HVEM at Kyoto (1977) , 'High Voltage Electron Microscopy', 1977, p. 159.
[56] 桐谷道雄,吉田直亮,電子顕微镜,10(1975) .95. 桐谷道雄,日本金属学会報,17(1978) ,646.
[57] Kiritani, M., Yoshida, N., Tabata,. H. and Maehara, Y., J. Phys. Soc. Jap., 38 (1975) , 1677.
[58] Kiritani, M., Proc. Int. Conf. Fund. Aspect of Rad. Damage in Metalt Gatlinburg (1975) , p. 695.
[59] Yoshida, N. and Kiritani, M., J. Phys. Soc. Jap., 35 (1973) , 1418.
[60] Kiritani, M. and Yoshida, N., J. Phys. Soc. Jap., 36 (1974) , 613. <
No related articles found!
No Suggested Reading articles found!