Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (1): 44-49    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF W AND Co ON HIGH TEMPERATURE CREEP BEHAVIOUR OF Ni-20Cr BASE ALLOYS
Yang Nansen; Wei Yuhuan; Fu Hongzhen and Zt Wengao (Central Institute of Iron and Steel Research; Ministry of Metallurgical Industry) and Tang Rongde (Pushun Steel Works)
Cite this article: 

Yang Nansen; Wei Yuhuan; Fu Hongzhen and Zt Wengao (Central Institute of Iron and Steel Research; Ministry of Metallurgical Industry) and Tang Rongde (Pushun Steel Works). INFLUENCE OF W AND Co ON HIGH TEMPERATURE CREEP BEHAVIOUR OF Ni-20Cr BASE ALLOYS. Acta Metall Sin, 1981, 17(1): 44-49.

Download:  PDF(371KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The steady state creep behaviour of the Ni-20Cr base alloys with various contents of W and Co has been investigated in the temperature range of 940 to 1040℃. Both W and Co may raise the activation energy for creep, Qo, obeyed the relationship:Q_c=Ae~(kx/lg~(?)) where x is the atomic fraction of W or Co additions; A is a constant for the alloy composition and k is equal to 7.0 and 0.55 for W and Co additions respectively. The steady state creep rate (?)_s of Ni-Cr-Co-W alloys was predicated to be:(?)_s=Cσ~m exp (-Q_e/RT) where m=6.45±0.10 or 5.3 depending on whether μ phase is present or not. It was also shown that the (?)_s varies with the stacking fault energy γ according to the correlation:(?)_s∞γ~(1.4)
Received:  18 January 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I1/44

[1] 陈篪,邓枝生,吴伯群,丁树深,物理学报,23(1974) ,69.屯王
No related articles found!
No Suggested Reading articles found!