Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (1): 20-122    DOI:
Current Issue | Archive | Adv Search |
CRYSTALLOGRAPHIC ORIENTATION AND ELEMENTAL SEGREGATION OF FLAKES IN STEELS
Chen Lian and Liu Minzhi (Institute of Metal Research; Academia Sinica)
Cite this article: 

Chen Lian and Liu Minzhi (Institute of Metal Research; Academia Sinica). CRYSTALLOGRAPHIC ORIENTATION AND ELEMENTAL SEGREGATION OF FLAKES IN STEELS. Acta Metall Sin, 1981, 17(1): 20-122.

Download:  PDF(2657KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation on the crystallographic orientation and elemental segregation of flakes (hairline cracks) has been carried out by means of etching method and electron optical techniques (SEM, TEM, EPMA and AES). The results obtained are as follow:(1) The microappearances of fracture surface of flakes are a mixed fracture mode of quasicleavages and intergranular tearing waves.(2) The direction of the crack propagation of flakes are mostly along {112} planes of ferrite. These planes are also quasicleavage facets. While the orientation of the dendritic surface of flakes are {111} planes.(3) There are positive segregations of P, Mn, Mo, Cr and Si on the fracture surface of flakes, among which the most one is phosphorus.
Received:  18 January 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I1/20

[1] Heller, W., Weber, L., Hammerschmid, P. und Schweitzer, R., Stahl Eisen, 92 (1972) , 934.
[2] 陈廉、徐永波,尹万全,金属学报,14(1978) ,253.
[3] 陈廉、刘民治、张维斗、刘盛炎、尹万全、胡魁毅、孙继红,金属学报,15(1979) ,446,
[4] 罗阳,金属学报,13(1977) ,93.
[5] 大谷南海男,金属塑性腐食反应,产业图书,1972,p.172;194.
[6] Wallace, J. P., Scr. Met., 12 (1978) , 791.
[7] Heady,R.B.,Corrosion,34(1978) ,303.
[8] 冯端、王业宁、丘第荣,金属物理(上册)科学出版社,1964,p.19.
[9] Tien, J. K., Effect of Hydrogen on Behavior of Materials, ed. by Anthony W. Thompson, I. M. Bernstein, TMS-AIME, New York, 1976, p. 309.
[10] Troiano, A. R., Trans. ASM, 52(1960) , 54.
No related articles found!