IDENTIFICATION OF Fe_2 P IN PHOSPHIDE EUTECTIC OF CAST IRON
Liu Sen (Leshan Metallurgical Machine Works)
Cite this article: 

Liu Sen (Leshan Metallurgical Machine Works). IDENTIFICATION OF Fe_2 P IN PHOSPHIDE EUTECTIC OF CAST IRON. Acta Metall Sin, 1981, 17(1): 108-109.

Download:  PDF(766KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 January 1981     