Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (1): 1-114    DOI:
Current Issue | Archive | Adv Search |
GRAIN BOUNDARY EMBRITTLEMENT BY μ AND σ PHASES IN IRON-BASE SUPERALLOYS
Chen Guoliang; Xie Xishan; Ni Kequan; Xu Zhichao; Wang Di (Beijing Institute of Iron and Steel Technology); Zhang Ming (Shanghai Institute of Iron and Steel Research); and Ju Yuying (Shanghai No. 5 Steel Works)
Cite this article: 

Chen Guoliang; Xie Xishan; Ni Kequan; Xu Zhichao; Wang Di (Beijing Institute of Iron and Steel Technology); Zhang Ming (Shanghai Institute of Iron and Steel Research); and Ju Yuying (Shanghai No. 5 Steel Works). GRAIN BOUNDARY EMBRITTLEMENT BY μ AND σ PHASES IN IRON-BASE SUPERALLOYS. Acta Metall Sin, 1981, 17(1): 1-114.

Download:  PDF(2144KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Grain boundary embrittlement by μ and σ phases was studied in 15Cr-25Ni and 15Cr-40Ni type iron-base superalloys. The embrittlement of iron-base superalloys can be sensitive to small amounts of μ and σ phases present at the grain boundaries, even when the weight fraction is between 0.01 and 1%. The degree of embrittlement was found to be directly proportional to the concentration coefficients of the μ and σ phases at the grain boundaries. The embrittlement effect results in intergranular fracture during impact testing. Fracture mechanisms caused by the μ and σ phases were quite different. This embrittlement effect was suppressed by reducing the grain size or by decreasing or removing the grain boundary embrittling μ and σ phases by controlling the chemical composition of the alloys.
Received:  18 January 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I1/1

[1] Sullivan, C. P. and Donachie, M. J., Jr., Metals Eng. Quart.,11(1971) , № 4, 1.
[2] Decker, R.F. and Floreen, S., Precipitation from Iron-Base Alloys, Eds. G. R. Speich and J. B. ClarK,Gordon and Breach, New York, 1965, p. 69.
[3] Sims, C. T., J. Metals, 18 (1966) , 1119.
[4] Sabol, G, P, and Stickler, R., Phys. Status Solidi, 35 (1969) , 11.
[5] Sims, C. T., The Superalloys, Eds. C. T. Sims and W. C. Hagel, John Wiley & Sons, New York 1972, p. 259.
[6] Sullivan, C. P. and Donachie, M. J., Jr., Metals Eng. Quart., 7 (1967) ,№ 1, 36.
[7] Mihalisin, J. R., Bieber, C. G. and Grant, R. T., Trans. AIME, 242 (1968) , 2399.
[8] 陈淦生、姚常春、仲增墉,金属学报,14(1978) ,284.
[9] Beattie, H. J., Jr., and Hagel, W. C., Trans. AIME, 221 (1961) , 28.
[10] Maniar, G. N., Muzyka, D. R. and Whitney, C. R., Trans. AIME, 245 (1969) , 701.
[11] Wood, J. R., Proe. 3rd Int'l Symp. on Superalloys, Seven Springs, Pa. 1976, p. 227.
[12] 北京钢铁学院高温合金研究组,金属学报,14(1978) ,440.
[13] 上海钢铁研究所,北京钢铁学院,15Cr-40Ni型铁基高温合金的研究报告,1978.
No related articles found!