THERMODYNAMICS OF THE MARTENSITIC TRANSFORMATION β(γ)→ε
Xu Zuyao (T. Y. Hsu) Shanghai Jiaotong University
Cite this article: 

Xu Zuyao (T. Y. Hsu) Shanghai Jiaotong University. THERMODYNAMICS OF THE MARTENSITIC TRANSFORMATION β(γ)→ε. Acta Metall Sin, 1980, 16(4): 430-434.

Download:  PDF(320KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The stacking-fault energy (SFE) at M_s temperature in Co, Co-14Ni and Co-3.5Cu alloys are given and the nucleation mechanism of ε-martensite is discussedwith respect to their driving forces. The transformation barrier in pole mechanismmight include the SFE of parent phase as well as the interaction energy betweenimperfect dislocations, the driving force pushes the dislocations to glide with aspeed about 0.4 of that of sound that provides the dynamic energy to overcomethe transformation barrier. The Seeger's pole mechanism may be effective for themetals with higher SFE like Co, but inavailable for the Co-14Ni and Co-3.5Cualloys with low SFE in 10~(-1) order of magnitude in which the spontaneous nu-cleation of fault will be applicable.
Received:  18 April 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I4/430

[1] Christian, J. W., Proc. Royal Soc., A206 (1951) , 51.
[2] Seeger, A., Z. Metallk., 44 (1953) , 247.
[3] Seeger, A., Z. Metallk., 47 (1956) , 653.
[4] Seeger, A., The Mechanism of Phase Transformations in Metals, Inst. Metals Monog. №18, 1956, p. 330.
[5] Bollmann, W., Acta Met., 9 (1961) , 972.
[6] Cohen, J. and Weertman, J., Acta Met., 11 (1963) , 996.
[7] Olson, G. B. and Cohen, M., Met. Trans., 7A (1976) , 1897.
[8] 徐祖耀、陆明炯,钴及其合金马氏体相变热力学,上海交通大学,1966.
[9] 陆明炯,上海交通大学研究生毕业论文,1965.
[10] Sato, A., Sunaga, Y. and Mori, T., Acta Met., 25 (1977) , 627.
[11] Ericsson, T., Acta Met., 14 (1966) , 853.
[12] Friedel, J.,Dislocations, Pergamon Press, 1964, p. 166.
[13] Siems, R., Delavignette, P. und Amelinckx, S., Z. Phys., 165 (1961) , 502.
[14] Seeger, A., Handbuch der Physik, Band Ⅶ/Ⅰ, Hrsg. S. Flugge, Springer, Berlin, 1955, p, 383.U
No related articles found!
No Suggested Reading articles found!