THERMODYNAMICS OF THE MARTENSITIC TRANSFORMATION IN Fe-X-C SYSTEMS
Xu Zuyao (T. Y. Hsu) Shanghai Jiaotong University
Cite this article: 

Xu Zuyao (T. Y. Hsu) Shanghai Jiaotong University. THERMODYNAMICS OF THE MARTENSITIC TRANSFORMATION IN Fe-X-C SYSTEMS. Acta Metall Sin, 1980, 16(4): 426-429.

Download:  PDF(301KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The △G_(Fe-X-C)~(γ→α) in the martensitic transformation in Fe-X-C system is sugges-ted as: △G_(Fe-X-C)~(γ→α)=x_(Fe)△G_(Fe-X-C)~(γ→α)+x_C RT lnγ_C~α/γ_C~γ+x_i△G_i~(γ→α) +△Ω~(γ→α)where γ_C~α and γ_C~γ are activity of carbon in Fe-X-C ferrite and austenite respec-tively. The M_s of Fe-Ni-C and Fe-Cr-C obtained in present work are in goodagreement with the experimental results, showing that the above equation inavailable and convenient for application. The M_s of Fe-X-C system mainlydepends upon the activity of carbon in Fe-X-C and the strengthening effect onaustenite and carbon play an important role to determine the driving force of themartensite transformation in Fe-X-C.
Received:  18 April 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I4/426

[1] Fisher, J. C., Trans. AIME, 185 (1949) , 688.
[2] Rao, M. M., Russell, R. J. Winchell, P. G., Trans. AIME, 239 (1967) , 634.
[3] 徐祖耀,金属学报,15(1979) ,329.
[4] 徐祖耀,金属学报,16(1980) ,420
[5] Schoen, F. J. and Owen, W. S., Met. Trans., 2 (1971) , 2431.
[6] Wada, T., Wada, H., Elliott, J. F. and Chipman, J., Met. Trans., 2 (1971) , 2199.
[7] Wada, T., Wada, H., Elliot, J. F. and Chipman. J., Met. Trans., 3 (1972) , 2865.
[8] Swartz, J. C., Trans. AIME, 245 (1969) , 1083.
[9] Labo, J. A. and Geiger, G. H., Met. Trans., 7A (1976) , 1347.
[10] Kaufman, L., Clougherty, E. V. and Weiss, R. J., Acta Met., 11 (1963) , 323.
[11] Goodenow, R. H. and Hehemann, R. F., Trans. AIME, 233 (1965) , 1777.
[12] Rao, M. M. and Winchell, P. G., Trans. AIME, 239 (1967) 956.
[13] Magee, C. L. and Davies, R. G., Acta Met., 19 (1971) , 345.
[14] Yeo, R. B. G., Trans. AIME, 227 (1963) , 884.
[15] Steven, W. and Haynes, A. G., J. Iron Steel Inst. 183 (1956) , 349.
[16] Lyman, T. and Troians, A. R., Trans. Amer. Soc. Metals, 37 (1946) , 402.
[17] Owen, W. S., Wilson, E. A. and Bell, T., High Strength Materials, Ed. by V. F. Zackay, Wiley, N. Y., 1965, p. 185.
[18] Andrews, K. W., J. Iron Steet Inst. 203 (1965) , 721.
[19] Bodsworth, C., Davidson, I. M. and Atkinson, D., Trans. AIME, 242 (1968) , 1135.
No related articles found!
No Suggested Reading articles found!