GLIDE DEFORMATION OF METALLIC GLASSES UNDER CONCENTRATE LOADING
Patu;Su Huihe Institute of Metal Research; Academia Sinica
Cite this article: 

Patu;Su Huihe Institute of Metal Research; Academia Sinica. GLIDE DEFORMATION OF METALLIC GLASSES UNDER CONCENTRATE LOADING. Acta Metall Sin, 1980, 16(3): 368-386.