| CALCULATION ON THE STABILITY OF THE CONSTANT PERMEABILITY ALLOY |
| Yang Yingshan;Zhang Anning Central Iron and Steel Research Institute; Ministry of Metallurgical Industry |
|
Cite this article:
Yang Yingshan;Zhang Anning Central Iron and Steel Research Institute; Ministry of Metallurgical Industry. CALCULATION ON THE STABILITY OF THE CONSTANT PERMEABILITY ALLOY. Acta Metall Sin, 1979, 15(4): 489-497.
|
|
|
Abstract A study was made to calculate the stability of permeability of isopermalloyrelated to the magnetocrystalline anisotropy with the aid of a computer. It wouldseem that the problem regarding the correlation of magnetization with magneticfield intensity might be solved by a non-existence of analytical form, sinβ=f(H),and of the condition of many values. Therefore, the stability of an alloy char-acterized by an evenly random crystal orientation may be much superior to thatby an arbitrary texture.
|
|
Received: 18 April 1979
|
[1] Bozorth, R. M., Ferromagnetism, D. Van Nostrand, London, 1951. p. 579. [2] 杨膺病善,王振昌,王崇愚,陈新华,金属学报11(1975) ,196. [3] Taniguchi, S., Sci. Rep. Res. Inst. Tohoku Univ., Ser. A, 8 (1956) , № 3, p. 173. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|