| THE IMMUNIZATION OF FLAKES IN A MEDIUM CARBON MANGANESE STEEL BY HOT WORKING |
| Chen Lian;Liu Minzhi(Liu Min-chih);Zhang Weidou;Liu Shengyen;Yin Wanquan;Hu Kuiyi;Sun Jihong |
|
Cite this article:
Chen Lian;Liu Minzhi(Liu Min-chih);Zhang Weidou;Liu Shengyen;Yin Wanquan;Hu Kuiyi;Sun Jihong. THE IMMUNIZATION OF FLAKES IN A MEDIUM CARBON MANGANESE STEEL BY HOT WORKING. Acta Metall Sin, 1979, 15(4): 446-576.
|
|
|
Abstract 42Mn2 steel cylinders processed by hot extrusion and drawing of flake-con-taining billets have been examined by SEM and by other methods to ascertain theimmunization of flakes in the final products. All internal flakes in the billets werecompletely healed after processing into cylinders, with the exception of those origi-nally exposed to the surface of the billet owing to oxidation. From practical appli-cation point of view, however, little difference in properties has been found betweencylinders completely or incompletely immunized from flakes. Thus, in the fatiguetest of the cylinders within cyclic stress ranges of 10?150 kg/cm~2, no signalsinduced by the formation and propagation of cracks were detected by acoustic emis-sion till 30,000-60,000 cycles. Likewise, the static bursting test of all cylindersalso met the standard set up by the users.
|
|
Received: 18 April 1979
|
[1] Дубовой.В.Я.钢中的白点,杨惠毕译,重工业出版社,1954年. [2] Koehler, E. L. and Wischar, H. B., ASM Trans. Quart., 40 (1948) , 513. [3] (1958) , № 1, 67. [4] Склюев,П.В.,大型锻件中的氢和白点,陈洵,曾祖良,张同和合译,机械工业出版社,1966年,p.98. [5] Hewitt, J. and Murray, J. D., Metal. Constr. Brit. Weld. J., 1 (1969) , № 2, 24. [6] 陈廉,徐永波,尹万全,金属学报,14(1978) ,253. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|