A MODIFIED DOUBLE CANTILEVER BEAM MODEL FOR DETERMINING K_(Ic)
Dong Xuemin Central Iron and Steel Research Institute; Ministry of Metallurgical Industry
Cite this article: 

Dong Xuemin Central Iron and Steel Research Institute; Ministry of Metallurgical Industry. A MODIFIED DOUBLE CANTILEVER BEAM MODEL FOR DETERMINING K_(Ic). Acta Metall Sin, 1979, 15(3): 392-399.

Download:  PDF(523KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified model of double cantilever beam in determining K_(IC) has been pro-posed. In our model the behaviour of the double cantilever beam specimen ischaracterized by a constant stress intensity factor on condition that cracks in thespecimen propagate under constant displacement conditions. Results obtained froma 4340 steel appear to be in reasonable agreement with the established data.
Received:  18 March 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I3/392

[1] Mostovoy. C. et al., J. Mater. Sci., 2 (1967) . 661.
[2] Raasch, J., Int. J. Fract. Mech., 7 (1971) , 289.
[3] Kanninen, M. F., Int. J. Fract., 10 (1974) , 415.
[4] 杜庆华,材料力学,人民教育出版社,1961,p.197.
No related articles found!
No Suggested Reading articles found!