| EFFECT OF SILICON ON THE TRANSITION OF BRITTLENESS IN A NICKEL BASE WROUGHT SUPERALLOY |
| Wang Yunshi;Bi Jing;Guan Xuemin;Zhang Xizhang;Wang Jingyun;Lin Shuzhi;Xu Anshuang |
|
Cite this article:
Wang Yunshi;Bi Jing;Guan Xuemin;Zhang Xizhang;Wang Jingyun;Lin Shuzhi;Xu Anshuang. EFFECT OF SILICON ON THE TRANSITION OF BRITTLENESS IN A NICKEL BASE WROUGHT SUPERALLOY. Acta Metall Sin, 1979, 15(3): 339-443.
|
|
|
Abstract The tensile strength, ductility or impact value of a wrought nickel base super-alloy Ni-15Cr-6W-3Mo-2Al-2Ti depend markedly upon the silicon content of thealloy. On plotting these mechanical properties vs the silicon content which rangesfrom 0.1 to 0.89%, a saddle shown by the existence of a minimum at about 0.4-0.6% Si occurs. There is reason to believe that such a saddle behavior may be caus-ed by the variation of mechanical properties with the type, amount and morpho-logy of carbides as well as with the sequence of carbide precipitation in the alloyas influenced by its silicon content. Thus, the amount of M_6C and M_(23)C_6 precipi-tated along the grain boundaries would appear to proceed in four stages as follows: 1. For silicon content up to 0.1%, globular M_(23)C_6 may be the sole type ofcarbide formed; 2. In the range from 0.1 to 0.4% Si, besides M_(23)C_6, M_6C begins to appearand increases with increase of silicon content. The morphology of the carbidesseems to be different, however, being in a discontinuous, blocky form; 3. In the range from 0.4 to 0.6% Si, continuous films of M_6C were present.As might be expected, this type of carbide is very detrimental to the tensile andimpact properties at room temperature. The precipitation of M_(23)C_6 was slowed downor even suppressed; 4. In the range from 0.6 to 0.89% Si, M_6C may be altered to discontinuous,blocky form, whereas M_(23)C_6 may be very much limited. In conclusion, the detrimental effect of carbide is mainly associated with itsfilm-like morphology especially along the grain boundaries. Of course, carbides ingranular form are good strengtheners. According to prevailing view, criterion for the formation of either M_6C orM_(23)C_6 in nickel base superalloys would seem to be the relative Mo and W con-tents, e. g. if Mo+1/2W>6%, M_6C will be formed. Present work indicates that si-licon plays as equally important role in the formation of M_6C besides the Mo andW contents of the wrought nickel base superalloys.
|
|
Received: 18 March 1979
|
[1] Miner, R. V., Met. Trans., 8A (1977) , 1949. [2] Betteridge, W. and Heslop, J., The Nimonic Alloys; and Other Nickel-Base High-Temperature Alloys, 2nd ed., Edward Arnold, London, 1974, p. 23. [3] Eieselstein, H. L., Advance in the Technology of Stainless Steels and Related Alloys, ASTM, Phil., 1965, p. 78, (Disc.). [4] Rizzo, F. J. and Buzzanell, J. D., J. Metals, (1969) , № 10, 24. [5] Sakakiara, M. and Sekino, S., Superalloys processing; Proceedings of the 2nd International Conference, 1972, Champion, Pa., New York, AIME, P. I-1. [6] 待发表工作. [7] Douglass, D. L. and Armizo, J. S., Oxid. Metals, 2 (1970) , 207. [8] Savage, W. F. and Krantz, B. M., Weld. J. (New York), 50 (1971) , 292-S. [9] Yeniscarich, W. and Fox, C. W., Effect Minor Element on the Weldability of High Nickel Alloys, WRC, N. Y., 1969, p. 24. [10] Preis, G. und Lennartz, G., Arch. Eisenhuettenw., 8 (1975) , 509. [11] Piearcey, B. J. and Smashey, R. W., Trans. AIME, 239 (1967) , 451. [12] Sims, C. T., J. Metals, 18 (1966) , 1119. [13] Dreshfield, R. L., ASM Trans. Quart., 61 (1968) , 352. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|