| BENEFICIATION OF DIASPORE-KAOLINITE-BEARING BAUXITE BY FLOTATION |
| Li Yuewu;Chen Dong Shenyang Designing Institute of Aluminum and Magnesium Industry |
|
Cite this article:
Li Yuewu;Chen Dong Shenyang Designing Institute of Aluminum and Magnesium Industry. BENEFICIATION OF DIASPORE-KAOLINITE-BEARING BAUXITE BY FLOTATION. Acta Metall Sin, 1979, 15(3): 319-322.
|
|
|
Abstract Results of the beneficiation of the diaspore-kaolinite-bearing bauxite by flota-tion, from laboratory and small-scale continuous processing to pilot plant testingare described. Using raw materials with initial Al_2O_3/SiO_2 ratio of 4.6-5, theflotation concentrates finally attained a ratio greater than 8 with a recovery of Al_2O_3amounting to 70-80%. Results of digesting test for producing alumina by Bayer process, as well astests for making comprehensive utilization of the flotation tailings are also presen-ted.
|
|
Received: 18 March 1979
|