AN EXPRESSION FOR CALCULATING CRACK EXTENSION
Zhao Tingshi Central China Engineering Institute
Cite this article: 

Zhao Tingshi Central China Engineering Institute. AN EXPRESSION FOR CALCULATING CRACK EXTENSION. Acta Metall Sin, 1979, 15(2): 296-298.