| EFFECT OF CERTAIN ALLOYlNG ELEMENTS ON THE MECHANICAL PROPERTIES OF A WROUGHT NICKEL-IRON BASE SUPERALLOY |
| Wang Yunshi;Wang Sukun;Zhang Shunnan;Zhao Yucai;Li Shijin |
|
Cite this article:
Wang Yunshi;Wang Sukun;Zhang Shunnan;Zhao Yucai;Li Shijin. EFFECT OF CERTAIN ALLOYlNG ELEMENTS ON THE MECHANICAL PROPERTIES OF A WROUGHT NICKEL-IRON BASE SUPERALLOY. Acta Metall Sin, 1979, 15(2): 187-196.
|
|
|
Abstract The effects of certain alloying elements such as titanium, aluminium, molyb-denum, carbon, boron, etc. on the tensile, impact and stress-rupture propertiesof a 42Ni-35Fe-13Cr superalloy have been investigated. Titanium or molybdenumincreased the 0.2% proof stress, the elongation, and the impact properties at roomtemperature as well as the stress-rupture life of the alloy at elevated temperatures.The presence of aluminium up to 0.3% accelerated the formation of γ'-Ni_3 (Ti, Al).Carbon and boron promoted the formation of fine grain size, with an optimumat 0.035% C and 0.010% B, where a maximum stress-rupture life of such analloy was obtained. The strengthening mechanism of the above alloying elementsand their optimum contents are discussed. It is emphasized that a close controllof the carbon and boron contents of the alloy and demand of high quality andcleanness of the ingot are particularly important.
|
|
Received: 18 February 1979
|
[1] Kirman, I. and Warrington, D. H., J. Inst. Metals, 99 (1971) , 197. [2] Guimier, A. and Strudel, J. L., Proceedings of the Second International Conference on the Strength of Metals and Alloys, 1970, Vol. Ⅲ, ASM, Ohio, p. 1145. [3] Decker, R. F. and Floreen, S., Precipitation from Substitutional Iron-Base Austenitic and Martensitic Solid Solutions, Precipitation from Iron-Base Alloys, 1965, AIME, New York. [4] Irvine, K. L., J. Iron Steel Inst. London, 199 (1961) , 1953. [5] 王允实等,待发表工作. [6] Holt, R. T. and Wallace, W., Int. Met. Rev., 3 (1976) , 1. [7] Stroup, J. P. and Pugliese, L. A., Met. Progr., 2 (1968) , 96.R |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|