| AN INVESTIGATION OF THE DIRECTIONAL SOLIDIFICATION OF A NICKEL-BASE SUPERALLOY |
| Lin Dongliang;Lin Tung-liang;Yao Deliang Shanghai Jiaotong University |
|
Cite this article:
Lin Dongliang;Lin Tung-liang;Yao Deliang Shanghai Jiaotong University. AN INVESTIGATION OF THE DIRECTIONAL SOLIDIFICATION OF A NICKEL-BASE SUPERALLOY. Acta Metall Sin, 1979, 15(2): 177-303.
|
|
|
Abstract The structure and properties of a directionally solidified high strength castnickel-base superalloy have been studied. Directional solidification significantly in-creased the resistance to thermal-fatigue and intermediate temperature rupture lifeas well as the ductility and the tensile strength and high temperature rupture lifeof the alloy. The improvement of rupture life at certain intermediate temperature(about 760℃) was found to be due to an extension of the secondary stage ofcreep, whereas at a high temperature (about 980℃) the same improvementcame from an extension of the tertiary stage. The absence of grain boundaries inthe transverse direction gave rise to better mechanical properties, in particular, the<100> preferred orientation of the columnar grains played an important part inthe increased strength at elevated temperatures. The secondary creep rate was lowered and the second creep stage extendedafter high temperature solution treatment. This was found to be due to the solu-tioning of the coarse γ' phase on heating and the subsequent reprecipitation of auniformly dispersed fine γ' particles in the cast alloy after cooling. In the above directionally solidified alloy, primary MC carbides seem to serveas the sites for creep and thermal-fatigue crack initiation. This rather suggests thatthe high temperature mechanical properties of the alloy may possibly be furtherimproved if its carbon content is lowered.
|
|
Received: 18 February 1979
|
[1] Piearcey, B. J. Kear, B. H. and Smashey, R. W., Trans. ASM, 60 (1967) , 634. [2] Piearcey, B. J. and Terkelsen, B. E., Trans. AIME, 239 (1967) , 1143. [3] VerSnyder, F. L, and Shank, M. E., Mater. Sci. Eng., 6 (1970) , 213. [4] VerSnyder, F. L., Proceedings of the Second Conference on the Strength of Metals and Alloys, 1970, Vol. Ⅱ, ASM, Ohio, p. 1011-1027. [5] Lund, C. H., Found. Trade J., 128 (1970) , 815. [6] Leverant, E. R. and Duhl, D. N,. Met. Trans., 2 (1971) , 907. [7] Duhl, D. N., Erickson, J. S. and Sullivan, C. P., Metal Progr., 103 (1973) , 38. [8] Northwood, J. E. and Homewood, T., Met. Metal Form., 41 (1974) , 254. [9] woodford, D. A. and Frawley, J. J., Met. Trans., 5 (1974) , 2005. [10] 中川幸也,大友晓,杂贺喜规,石川岛播磨技报,15 (1975) , 574. [12] 中川奉也,村上和夫,大友 晓,深川宗元,杂贺喜规,石川岛播磨技报17(1977) ,467. [13] Sims, C. T. and Hagel, W. C., The Superalloys, Wiley, New York, 1972. [14] Jackson, J. H., Met. Trans., 8A (1977) , 1615. [15] 林栋粱,王来生,高温固溶处理对提高定向凝固镍基高温合金蠕变强度的作用(待发表). |
| No Suggested Reading articles found! |
|
|