| A BRIEF ACCOUNT OF THE CONSTRUCTION AND THERMOTECHNICAL PERFORMANCE OF A TOP-FIRED STOVE |
| Liu Dehua;Shao Jingwen Institute of Chemical Metallurgy; Academia Sinica |
|
Cite this article:
Liu Dehua;Shao Jingwen Institute of Chemical Metallurgy; Academia Sinica. A BRIEF ACCOUNT OF THE CONSTRUCTION AND THERMOTECHNICAL PERFORMANCE OF A TOP-FIRED STOVE. Acta Metall Sin, 1979, 15(1): 39-43.
|
|
|
Abstract The thermotechnical performance and construction of a new type top-firedstove shown in this paper are better than internal and external combustion cham-ber stoves, and therefore it may be adaptable to high top pressures and high tem-peratures blast furnaces. The stove construction may also be suitable for rebuildingthe existing internal combustion chamber stoves, as well as for designing hot blaststoves for high blast temperatures and high pressures. Reasonable approach to theconstruction and arrangement of the top-fired stoves has been suggested.
|
|
Received: 18 January 1979
|
[1] Jansen, H. W. and Hilger, H. J., Blast Furn. Steel Plant, 58 (1970) , 171. [2] 刘德华,邵景文,“云南磷肥厂顶燃式热风炉的初步设计及热工计算”,中国科学院化工冶金研究所资料,1978年4月. [3] 云南磷肥厂,“高炉法冶炼黄磷阶段小结”,1972年3月. [4] Larr, J. van, Ironmaking Proceedings, Vol. 33, Atlantic City, 1974, p. 408. [5] Higuchi, M., Shibuya, T. and Niwa, Y., Ironmaking Proceedings, Vol. 34, Toronto, 1975, p. 542. [6] 高成渤等,“高炉热风炉道系统之热量损失”,鞍钢中央试验室,1957年4月. [7] Petit, D., Iron Steel Eng., 41 (1964) , № 11, 175 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|