| A FLUID-DYNAMICAL LOWER DENSITY SIMULATION TEST FOR LD CONVERTER |
| Li Disheng;Han Ren;Xie Chuanshu Research Institute of Wuhan Iron and Steel Company |
|
Cite this article:
Li Disheng;Han Ren;Xie Chuanshu Research Institute of Wuhan Iron and Steel Company. A FLUID-DYNAMICAL LOWER DENSITY SIMULATION TEST FOR LD CONVERTER. Acta Metall Sin, 1979, 15(1): 12-22.
|
|
|
Abstract Applying the similarity theory based upon the behaviour of the supersonicoxygen jet of 2.12 and 1.465 Mach respectively and upon its interaction withthe bath, certain simulation tests for 50-ton LD converter have been carried out. Incase of geometry and boundary condition similarities, a new test, the so called"lower density simulation", has been proposed to realize not only the jet dynam-ics but also its interaction with bath. In all, five tests simulating the jet dynam-ics behaviour under various conditions, its interaction with bath, the inlluenceof fluid dynamics on rate of carburization in bath, etc. were conducted. The rel-iability of such lower density simulation tests for LD converter was subjected totheoretical analysis and further verified by experimental results obtained by NACA.
|
|
Received: 18 January 1979
|
[1] Chatterjee, A. and Bradshaw, A. V., J. Iron Steel Inst., 210 (1972) , 179. [2] Robertson, A. D. and Sheridan, A. T., J. Iron Steel Inst., 208 (1970) , 625, [3] Suri, A. K. and Bose, D. K., Met. Trans., 5 (1974) , 463. [4] 下间照男,佐野和夫,铁钢,51(1965) ,752. [5] ibid, 51 (1965) , 1909. [6] Banks, B., J. Fluid Mech., 15 (1963) , 13. [7] Chatterjee, A., Iron Steel (London), 46 (1973) , 38. [8] Ферри,А.,超音速空气动力学,郭进达,巢以明译,1959,国防出版社,101. [9] Shapiro, H., Dynamics and Thermodynamics of Compressible Fluid Flow, Vol. Ⅱ, p. 696. [10] Chatterjee, A., Ironmaking Steelmaking, 3 (1976) , 21. [11] Chatterjee, A., Iron Steel (London), 45 (1972) , 627. [12] 北京大学等,本钢120吨转炉喷枪半测定,1975. [13] Thomas, T. L. and Aydelott, J. C., NASA TND-6368, 1--15. [14] Sears,W.R.,高速空气动力理论,安继光译,1960,国防出版社,38. [15] Tourgan, K. J. and Drake, R. M., Rarefied Gas Dynamics, Vol. Ⅱ, p. 402. [16] Kane, E. D. and Maslach, G. J., NACA TN 2210, (1950) , 1--37. [17] Sherman, F. S., NACA TN 2995, (1953) , 1--54. [18] Donalason, C. dup., NACA RM NoL8J14, (1948) , 1--21. [19] Thompason, P. A., Compressible Fluid Dynamics, 1971, p. 292. [20] Sohichi Inada and Tetsuya Watanabe, Trans. Iron Steel Inst. Japan, 17 (1977) , 59. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|