| DISTRIBUTION OF NODULARIZING ELEMENTS IN R. E. TREATED SPHEROIDAL GRAPHITE CAST IRONS |
| Han Qiyong;Wu Weijiang;Fang Keming;Lu Jing;Zhang Baojun;Xie Deyi;Pei Lixia Beijing Institute of Iron and Steel Technology |
|
Cite this article:
Han Qiyong;Wu Weijiang;Fang Keming;Lu Jing;Zhang Baojun;Xie Deyi;Pei Lixia Beijing Institute of Iron and Steel Technology. DISTRIBUTION OF NODULARIZING ELEMENTS IN R. E. TREATED SPHEROIDAL GRAPHITE CAST IRONS. Acta Metall Sin, 1979, 15(1): 1-187.
|
|
|
Abstract The distribution of nodularizing elements such as cerium, yttrium, magnesiumor calcium and of subversive such as sulphur in R. E. treated spheroidal graphitecast irons has been studied by means of autoradiograph, electron probe and ionmass microanalysis. The blackness of autoradiography to a first approximationshowed the content of the radioactive components in graphite and in matrix. Cer-tain graphite spherulites each contained a nucleus, the composition of which wasdifferent with different nodularizing elements. The distribution of the different nod-ularizing elements cerium, magnesium, yttrium, calcium and the subversive agentsulphur in nodular cast iron occurred in many different ways, compounds ofnodularizing elements might exist as nuclei of graphite spherulites with yttrium,magnesium and calcium etc. around them. In certain spherulites, cerium was found-to distribute uniformly but yttrium irregularly. In cast irons treated separately bycerium, yttrium or other nodularizing elements, however, hardly any rare earthwas found to enrich around most of the spherulites. In view of the complex be-havior in rare earth distribution, it would appear that graphite spherulites are form-ed far from only in a single way. The interaction due to the nodularizingelements in fact may be the result of scavenging subversives (sulphur, oxygen, etc.),in its consequence the surface tension of melt and the interfacial tension at themelt-graphite boundaries thus facilitating the formation of graphite spherulites.The mechanism of duplex graphite spherulites formation has also been primarilyexamined.
|
|
Received: 18 January 1979
|
[1] Hillert, M. and Lindblom, Y., J. Iron Steel Inst., 176 (1954) , 388. [2] (1971) , № 7, 36. [3] 12 (1961) , № 2, 233. [4] Spendler, W. A. and Flinn, R. A., Trans. Amer. Foundrymen's Soc., 70 (1962) . 1017. [5] Michael, A. B., J. Iron Steel Inst., 178 (1954) , № 2, 160. [6] 20 (1965) . № 2. 236. [7] 张博,山本悟,川野丰?,尾崎良平,日本金属学会志,41(1977) ,471. [8] 奥本武臣,饭岛史郎,铸物,35(1963) ,728. [9] 饭岛史郎,奥本武臣,铸物,38(1966) ,277. [10] Olette, M., Kohn, H., and Kozakevitch, P., Fonderie, (1965) , № 229, 87. [11] 4 (1957) , № 1, 177. [12] (1965) , № 4, 30. [13] Warrick, R. J., Trans, Amer. Foundrymen's Soc., 74 (1966) , 722. [14] Jacobs, M. H., Law, T. J., Melford, D. A. and Stowell, M. J., Metals Technol., 1 (1974) , № 11, 491. [15] Pirs, J., Microstruct. Sci., 3 (1975) , Pt. A, 91. [16] Katz, L. and Penfold, A. S., Rev. Mod. Phys., 24 (1952) , 28. [17] (1960) , 55. [18] Lux, B., Cast Metals Res., 8 (1972) , № 2, 49. [19] Mcswain, R. H. and Bates, C. E., The Metallurgy of Cast Iron, 1975, p. 423.
[20] Van Rooyen, G. T. and Paul, G., Metal Sci. J., 8 (1974) , 370. [21] Minkiff, I., Joint Conference on the Solidification of Metals. Brighton, 1967, Paper №. B/111/15. ISI Publication 110, 1968. [22] Zeedijk, H. B., J. Iron Steel Inst., 203 (1965) , 737. [23] 北京钢铁学院同位素小组,待发表工作. [24] Hunter, M. J. and Chadwick, G. A., J. Iron Steel Inst., 210 (1972) , 117. [25] 张博,山本悟,川野丰,尾崎良平,日本金属学会志,41(1977) ,464. [26] 张博,山本悟,川野丰,尾崎良平,日本金属学会志,41(1977) ,564,571. [27] Sadocha, J. P. and Grazleski, J. E., The Metallurgy of Cast Iron, 1975, p. 443. |